Invention Application
- Patent Title: Process for producing activated carbon for electrode of electric double-layer capacitor
- Patent Title (中): 双电层电容器电极活性炭生产工艺
-
Application No.: US11727974Application Date: 2007-03-29
-
Publication No.: US20070183958A1Publication Date: 2007-08-09
- Inventor: Takeshi Fujino , Shigeki Oyama , Naohiko Oki , Minoru Noguchi , Kenji Sato , Shushi Nishimura , Takashi Maeda , Yuji Kawabuchi , Takahiro Haga
- Applicant: Takeshi Fujino , Shigeki Oyama , Naohiko Oki , Minoru Noguchi , Kenji Sato , Shushi Nishimura , Takashi Maeda , Yuji Kawabuchi , Takahiro Haga
- Assignee: Honda Giken Kogyo Kabushiki Kaisha,Kuraray Chemical Co., Ltd.,Kashima Oil Co., Ltd.
- Current Assignee: Honda Giken Kogyo Kabushiki Kaisha,Kuraray Chemical Co., Ltd.,Kashima Oil Co., Ltd.
- Priority: JP11-226719 19990810; JP2000-24815 20000128; JP2000-195922 20000629; JP2000-234674 20000802; JP2000-024815 20000128
- Main IPC: C01B31/02
- IPC: C01B31/02

Abstract:
To produce activated carbon for an electrode of an electric double-layer capacitor, the following steps are carried out sequentially: a step of subjecting a massive mesophase pitch to a pulverizing treatment to provide a pulverized powder; a step of subjecting the pulverized powder to an infusibilizing treatment under conditions of a temperature in a range of 300° C. (inclusive) to 450° C. (inclusive) in the atmospheric air current, a step of subjecting the pulverized powder to a carbonizing treatment under conditions of a temperature in a range of 600° C. (inclusive) to 900° C. (inclusive) in an inert gas current to provide a carbonized powder, a step of subjecting the carbonized powder to an alkali activating treatment under conditions of a temperature in a range of 500° C. (inclusive) to 1,000° C. (inclusive) in an inert gas atmosphere, followed by the post treatments, thereby producing alkali-activated carbon, and a step of subjecting the alkali-activated carbon to a pulverizing treatment. If an electrode is produced using the activated carbon, the electrode density can be increased.