发明申请
- 专利标题: Zirconia Sintered Body and Production Method the Same
- 专利标题(中): 氧化锆烧结体和生产方法相同
-
申请号: US12866701申请日: 2009-02-06
-
公开(公告)号: US20110070441A1公开(公告)日: 2011-03-24
- 发明人: Shunji Mikaki , Kunihide Shikata
- 申请人: Shunji Mikaki , Kunihide Shikata
- 申请人地址: JP Kyoto-shi, Kyoto
- 专利权人: KYOCERA CORPORATION
- 当前专利权人: KYOCERA CORPORATION
- 当前专利权人地址: JP Kyoto-shi, Kyoto
- 优先权: JP2008-027694 20080207
- 国际申请: PCT/JP2009/052054 WO 20090206
- 主分类号: B32B5/16
- IPC分类号: B32B5/16 ; H01B1/02
摘要:
Provided are a zirconia sintered body that has excellent mechanical characteristics, as well as semiconductivity that can allow static electricity to escape at an appropriate rate, and a manufacturing method that can manufacture the same at lower cost than in the past. The zirconia sintered body is made of 66-90 parts by weight of zirconia that contains a stabilizer, and a total of 10-34 parts by weight of iron, chromium and titanium oxides. Of the iron, chromium and titanium oxides, the proportion of iron oxide is 70-99.5 wt %, the proportion of chromium oxide is 0.4-20 wt % and the proportion of titanium oxide is 0.1-10 wt %. The combined proportion of tetragonal and cubic crystals in the zirconia crystal phase is 90% or more and the mean crystal grain size of the zirconia is 0.3-0.5 μm. The mean crystal grain size of the iron, chromium and titanium oxides is 0.5-2.0 μm. It has excellent mechanical characteristics, as well as semiconductivity.
公开/授权文献
- US08383236B2 Zirconia sintered body and production method the same 公开/授权日:2013-02-26
信息查询