发明申请
US20130174949A1 AUSTENITIC HIGH MN STAINLESS STEEL AND METHOD PRODUCTION OF SAME AND MEMBER USING THAT STEEL
有权
奥氏体不锈钢不锈钢及其制造方法和使用该钢的成员
- 专利标题: AUSTENITIC HIGH MN STAINLESS STEEL AND METHOD PRODUCTION OF SAME AND MEMBER USING THAT STEEL
- 专利标题(中): 奥氏体不锈钢不锈钢及其制造方法和使用该钢的成员
-
申请号: US13824290申请日: 2011-09-29
-
公开(公告)号: US20130174949A1公开(公告)日: 2013-07-11
- 发明人: Masaharu Hatano , Shigeo Fukumoto , Hideki Fujii , Shinichi Ohmiya
- 申请人: Masaharu Hatano , Shigeo Fukumoto , Hideki Fujii , Shinichi Ohmiya
- 申请人地址: JP Tokyo
- 专利权人: NIPPON STEEL & SUMIKIN STAINLESS STEEL CORPORATION
- 当前专利权人: NIPPON STEEL & SUMIKIN STAINLESS STEEL CORPORATION
- 当前专利权人地址: JP Tokyo
- 优先权: JP2010-219396 20100929
- 国际申请: PCT/JP2011/073030 WO 20110929
- 主分类号: C21D8/10
- IPC分类号: C21D8/10 ; F16L9/02 ; F16K51/00 ; F17C1/00
摘要:
Inexpensive stainless steel and inexpensive and high strength stainless steel which has excellent hydrogen environment embrittlement resistance even if used in a hydrogen resistant environment in over 40 MPa high pressure hydrogen gas or a hydrogen resistant environment in liquid hydrogen, characterized by containing, by mass %, C: 0.1% or less, Si: 0.4 to 1.5%, Mn: 8 to 11%, Cr: 15 to 17%, Ni: 5 to 8%, Cu: 1 to 4%, and N: 0.01 to less than 0.15% and having a balance of Fe and unavoidable impurities, having a volume rate of δ-ferrite of 10% or less, and having a long axis of δ-ferrite before annealing of 0.04 to 0.1 mm.