- 专利标题: R-T-B SINTERED MAGNET AND PREPARATION METHOD THEREOF
-
申请号: US17244880申请日: 2021-04-29
-
公开(公告)号: US20210343459A1公开(公告)日: 2021-11-04
- 发明人: Yang LUO , Dunbo YU , Wei ZHU , Xinyuan BAI , Xiao LIN , Shengjie ZHU , Zilong WANG , Haijun PENG
- 申请人: GRIREM ADVANCED MATERIALS CO.,LTD. , Rare Earth Functional Materials (Xiong 'an) Innovation Center Co., Ltd. , Grirem (Rongcheng) Co., Ltd.
- 申请人地址: CN Beijing; CN Baoding; CN Weihai
- 专利权人: GRIREM ADVANCED MATERIALS CO.,LTD.,Rare Earth Functional Materials (Xiong 'an) Innovation Center Co., Ltd.,Grirem (Rongcheng) Co., Ltd.
- 当前专利权人: GRIREM ADVANCED MATERIALS CO.,LTD.,Rare Earth Functional Materials (Xiong 'an) Innovation Center Co., Ltd.,Grirem (Rongcheng) Co., Ltd.
- 当前专利权人地址: CN Beijing; CN Baoding; CN Weihai
- 优先权: CN202010366346.9 20200430
- 主分类号: H01F1/22
- IPC分类号: H01F1/22 ; H01F7/02 ; C22C38/00 ; C22C38/10 ; C22C38/06 ; C22C38/16 ; C22C38/14
摘要:
The present invention relates to an R-T-B sintered magnet and a preparation method thereof. The sintered magnet includes a grain boundary region T1, a shell layer region T2 and an R2Fe14B grain region T3; at 10 μm to 60 μm from a surface of the sintered magnet toward a center thereof, an area ratio of the shell layer region T2 to the R2Fe14B grain region T3 is 0.1 to 0.3, and a thickness of the shell layer region T2 is 0.5 μm to 1.2 μm; and an average coating percent of the shell layer region T2 on the R2Fe14B grain region T3 is 80% or more. In the present invention, by optimizing a preparation process and a microstructure of a traditional rare earth permanent magnet, diffusion efficiency of heavy rare earth in the magnet is improved, such that coercivity of the magnet is greatly improved, and manufacturing cost is reduced.