METALLOSILICATE CATALYST SOLVENT WASH
Abstract:
A method includes the steps of (a) contacting a solvent having a Water Solubility of 1 g or greater per 100 g of water with a metallosilicate catalyst having an alumina to silica ratio from 5 to 1500; and (b) heating the metallosilicate catalyst to a temperature from 125 C to 300 C fora period of 0.5 hours to 5 hours.