- 专利标题: COMPLEX-PHASE STEEL HAVING HIGH HOLE EXPANSIBILITY AND MANUFACTURING METHOD THEREFOR
-
申请号: US17762627申请日: 2020-09-25
-
公开(公告)号: US20220341010A1公开(公告)日: 2022-10-27
- 发明人: Chunsu LIU , Yulong ZHANG , Siliang ZHANG , Feng YANG , Yaping NI , Jintao WANG , Hanlong ZHANG , Ming WANG
- 申请人: BAOSHAN IRON & STEEL CO., LTD.
- 申请人地址: CN Shanghai
- 专利权人: BAOSHAN IRON & STEEL CO., LTD.
- 当前专利权人: BAOSHAN IRON & STEEL CO., LTD.
- 当前专利权人地址: CN Shanghai
- 优先权: CN201910920750.3 20190927
- 国际申请: PCT/CN2020/117724 WO 20200925
- 主分类号: C22C38/28
- IPC分类号: C22C38/28 ; C22C38/02 ; C22C38/04 ; C22C38/06 ; C22C38/26 ; C21D8/02 ; B21C47/02
摘要:
Disclosed in the present invention is complex-phase steel having high hole expansibility. The complex-phase steel has a microstructure of ferrite and bainite. The complex-phase steel having high hole expansibility comprises the following chemical elements in percentage by mass: C: 0.06-0.09%, Si: 0.05-0.5%, Al: 0.02-0.1%, Mn: 1.5-1.8%, Cr: 0.3-0.6%, Nb≤0.03%, Ti: 0.05-0.12%, and the balance of Fe and inevitable impurities. In addition, also disclosed in the present invention is a manufacturing method for the foregoing complex-phase steel having high hole expansibility. The method comprises the following steps: (1) smelting and casting; (2) heating; (3) hot-rolling; (4) phosphorous removal; (5) laminar cooling: a relaxation time period is controlled to be 0-8 s, and a laminar cooling rate is 40-70° C./s; (6) coiling; (7) leveling; and (8) pickling. The complex-phase steel having high hole expansibility can simultaneously satisfy the requirements for hole expansibility and good plasticity.