METHOD OF PREPARING ALKALI-ACTIVATED CEMENT BY STEPWISE CALCINATION WITH SODIUM CHLORIDE
摘要:
A method of preparing alkali-activated cement by stepwise calcination with sodium chloride includes the following steps. (1) Sodium chloride, a silicate and a carbonate are mixed and finely ground to obtain a raw material powder. (2) The raw material powder is calcined sequentially at 850-1050° C. and 1240° C. or more, and cooled to obtain a clinker. (3) The clinker is mixed with at least one of sodium hydroxide and potassium hydroxide, and ground finely to produce a cement powder.