发明授权
US5188667A Tungstic oxide-stannic oxide composite sol and method of preparing the
same
失效
氧化钨 - 氧化锡复合溶胶及其制备方法
- 专利标题: Tungstic oxide-stannic oxide composite sol and method of preparing the same
- 专利标题(中): 氧化钨 - 氧化锡复合溶胶及其制备方法
-
申请号: US795678申请日: 1991-11-21
-
公开(公告)号: US5188667A公开(公告)日: 1993-02-23
- 发明人: Yoshitane Watanabe , Keitaro Suzuki
- 申请人: Yoshitane Watanabe , Keitaro Suzuki
- 申请人地址: JPX Tokyo
- 专利权人: Nissan Chemical Industries, Ltd.
- 当前专利权人: Nissan Chemical Industries, Ltd.
- 当前专利权人地址: JPX Tokyo
- 优先权: JPX1-289410 19891107; JPX1-289542 19891107
- 主分类号: C01B13/14
- IPC分类号: C01B13/14 ; C01G19/02 ; C01G25/02 ; C01G30/00 ; C01G41/00 ; C03C17/23 ; C03C25/42 ; C04B41/50 ; C04B41/87 ; C09D7/12 ; D06M11/46 ; D06M11/48 ; D06P1/673 ; D21H17/67 ; D21H19/38 ; D21H21/22 ; D21H21/34 ; G02B1/10
摘要:
An aqueous sol of colloidal particles of tungstic oxide (WO.sub.3)-stannic oxide (SnO.sub.2) composite having a particle size of from 2 to 7 millimicrons is prepared by blending an aqueous solution of tungstic acid and an aqueous solution of an stannate in a weight ratio of from 0.5 to 100 as WO.sub.3 /SnO.sub.2. Where the WO.sub.3 -SnO.sub.2 composite sol in an amount of from 2 to 100 parts by weight as the total of WO.sub.3 and SnO.sub.2 is blended with a sol of a 3- to 5 valent metal oxide having a particle size of from 4 to 50 millimicrons in an amount of 100 parts by weight as the metal oxide, a modified metal oxide sol of colloidal particles having a size of 4.5 to 60 millimicrons as surface-coated with the tungstic oxide (WO.sub.3)-stannic oxide (SnO.sub.5) composite colloidal particles is prepared.