US6090734A Process for purifying clay by the hydrothermal conversion of silica impurities to a dioctahedral or trioctahedral smectite clay 失效
通过将二氧化硅杂质水热转化为二八面体或三八面体蒙脱石粘土来净化粘土的方法

Process for purifying clay by the hydrothermal conversion of silica
impurities to a dioctahedral or trioctahedral smectite clay
摘要:
A hydrothermal reaction which dissolves the amorphous silica and the crystalline silica impurities contained in a recovered, naturally occurring montmorillonite clay, and subsequently converts the dissolved silicas into a dioctahedral and/or trioctahedil smectite clay. The dissolution of silica is accomplished by adjusting the pH of an aqueous slurry of the recovered clay to a value of about 8.5 to about 10.0, preferably about 9.0 to about 9.5, at a temperature of at least about 150.degree. C., preferably about 180.degree. C. to about 250.degree. C., more preferably about 190.degree. C. to about 235.degree. C. Dissolved silica reacts with stoichiometric amounts of aluminum and/or magnesium and/or sodium added to the slurry, while at a temperature of at least about 150.degree. C., preferably about 185.degree. C. to about 250.degree. C., and at a pressure of at least about 200 bars, to synthesize a dioctahedral smectite clay from the dissolved silica; or the dissolved silica reacts with stoichiometric amounts of lithium and/or magnesium and/or sodium added to the slurry, at the same conditions, to form a trioctahedral smectite clay.
公开/授权文献
信息查询
0/0