发明授权
- 专利标题: Linear shape steel excellent in joint fatigue characteristics and production method therefor
- 专利标题(中): 线形钢具有优异的接头疲劳特性及其制造方法
-
申请号: US10018881申请日: 2002-05-06
-
公开(公告)号: US06706125B2公开(公告)日: 2004-03-16
- 发明人: Tatsumi Kimura , Yasushi Morikage , Keniti Amano , Takanori Okui , Keizou Taoka , Hironori Miura , Hiroyuki Ookubo , Fumimaru Kawabata
- 申请人: Tatsumi Kimura , Yasushi Morikage , Keniti Amano , Takanori Okui , Keizou Taoka , Hironori Miura , Hiroyuki Ookubo , Fumimaru Kawabata
- 优先权: JP2000-122323 20000424; JP2000-156273 20000526
- 主分类号: C22C3802
- IPC分类号: C22C3802
摘要:
When manufacturing a straight steel section having a joint 2 comprising a ball claw 21 and a curved claw 20 by hot-rolling a bloom vertically symmetrically to make a section blank having a flange 2A at a web 1 end (first step), vertically asymmetrically hot-rolling the section blank to adjust the size of the web and form the flange into a rough joint 2B including a projection 20A (second step), and subjecting the projection to hot bend rolling into a curved claw 20 (third step), wherein the bloom has a chemical composition comprising, in mass percentage, from 0.01 to 0.20% C, up to 0.8% Si, up to 1.8% Mn, up to 0.030% P, and up to 0.020% S; and therein the claw bending start temperature in the third step is a temperature of over Ar3 or up to Ar3-50° C., thereby achieving a depth of wrinkle flaws 10 present on the inner surface side of the curved claw of up to 0.5 mm.
公开/授权文献
信息查询