- 专利标题: Process for producing granular solid matter from coal ash as raw material and apparatus therefor
- 专利标题(中): 以煤灰为原料生产颗粒状固体物质的方法及装置
-
申请号: US12447235申请日: 2007-10-25
-
公开(公告)号: US08286900B2公开(公告)日: 2012-10-16
- 发明人: Noboru Takikawa , Yasunori Shibata , Atsushi Kondo , Tamaki Sakurai , Yoshiteru Kato , Kozo Kuga , Tomokazu Tengan , Tatsuya Ishihara , Atsushi Chinen , Yoshimichi Daijyo , Noboru Yasuda , Masahiko Doi
- 申请人: Noboru Takikawa , Yasunori Shibata , Atsushi Kondo , Tamaki Sakurai , Yoshiteru Kato , Kozo Kuga , Tomokazu Tengan , Tatsuya Ishihara , Atsushi Chinen , Yoshimichi Daijyo , Noboru Yasuda , Masahiko Doi
- 申请人地址: JP Kobe-shi JP Tokyo JP Kobe-shi
- 专利权人: Kawasaki Plant Systems Kabushiki Kaisha,Japan Coal Energy Center,Kawasaki Jukogyo Kabushiki Kaisha
- 当前专利权人: Kawasaki Plant Systems Kabushiki Kaisha,Japan Coal Energy Center,Kawasaki Jukogyo Kabushiki Kaisha
- 当前专利权人地址: JP Kobe-shi JP Tokyo JP Kobe-shi
- 代理机构: Marshall, Gerstein & Borun LLP
- 优先权: JP2006-289602 20061025
- 国际申请: PCT/JP2007/070810 WO 20071025
- 国际公布: WO2008/050831 WO 20080502
- 主分类号: B02C19/00
- IPC分类号: B02C19/00 ; B02C21/00
摘要:
A method of estimating the hydration reactivity of coal ash with high precision and determining the amount of milling water for obtaining a milling product in funicular form at the stage of milling; and a molding method being free from the problem of adhesion to a pressurization board at the stage of molding after the milling. When any collected coal ash exhibits a corrected basicity ((CaO+Fe2O3+MgO)/SiO2 (weight ratio)) of 0.1 or higher and a reactivity index (corrected basicity/(R2O/Al2O3) (weight ratio)) of 10 or higher, the coal ash as a raw ash is transferred to raw ash silo (2). Otherwise, the coal ash is transferred to waste ash silo (3). The raw ash within the raw ash silo (2) is poured in mill (8), and lime and gypsum are added and further milling water is charged thereto and milled. The amount of milling water is regulated so that with respect to agitator power per weight of material milled by the mill, the ratio of (average of power during 30 to 40 sec after completion of water charging)/(power at idling) ranges from 3 to 4, and so that with respect to agitator power per weight of material milled during 30 to 90 sec after completion of water charging, the ratio of (width of power fluctuation)/(average of power) ranges from 0.1 to 0.3.