Invention Grant
- Patent Title: Extraction process for reactive metal oxides
- Patent Title (中): 活性金属氧化物的提取工艺
-
Application No.: US10560515Application Date: 2004-06-11
-
Publication No.: US08834600B2Publication Date: 2014-09-16
- Inventor: Animesh Jha , Pailo Antony Malpan , Vilas Dattatray Tathavadkar
- Applicant: Animesh Jha , Pailo Antony Malpan , Vilas Dattatray Tathavadkar
- Applicant Address: GB Leeds
- Assignee: The University of Leeds
- Current Assignee: The University of Leeds
- Current Assignee Address: GB Leeds
- Agency: Dunlap Codding, P.C.
- Priority: GB0313886.4 20030616
- International Application: PCT/GB2004/002543 WO 20040611
- International Announcement: WO2004/113230 WO 20041229
- Main IPC: C22B9/00
- IPC: C22B9/00 ; B22D11/10 ; C21B7/14 ; C21B15/00 ; C21B3/04 ; C22B5/20 ; C22B11/10 ; C21B11/10 ; C01G49/02 ; C01F7/02 ; C01G15/00 ; C01F3/00 ; C01G23/047 ; C01G27/02 ; C01G25/02 ; C01B13/14 ; C01B33/12 ; C01B33/20 ; C01B15/14 ; C01B33/00 ; C22B21/00 ; C22B34/12 ; C01G49/06 ; C22B7/04 ; C22B1/02 ; C01F7/38 ; C01F7/14 ; C22B5/10

Abstract:
The present invention relates to a zero-waste process for extraction of alumina from different types of bauxite ores and red mud residues and of titanium dioxide from ilmenite. Iron oxide is first reduced to metallic iron above the melting point of C-saturated cast iron alloy which yields a high-C iron alloy and an Al and Ti metal oxide rich slag which is then treated with alkali carbonate to form alkali aluminates and titanates. The alkali aluminates are separated by water leaching from which the hydroxide of alumina is precipitated by bubbling C02. The residue from water leaching is treated with sulphuric acid and Ti02 is precipitated via a hydrolysis route. The process recovers most of the metal values and generates only small quantities of silicious residues at pH 4-5 which can be used for soil conditioning. The present also relates to a method for selective separation of Ti02-rich oxides from titaniferrous ore/residue materials via oxidative roasting in the presence of alkali carbonate or carbonates followed by aqueous leaching of the roasted material and selective precipitation of Ti02 under controlled condition below pH=4.