US09558872B2 R-T-B rare earth sintered magnet, alloy for R-T-B rare earth sintered magnet, and method of manufacturing the same
有权
R-T-B系稀土烧结磁体,R-T-B系稀土类烧结磁体用合金及其制造方法
- Patent Title: R-T-B rare earth sintered magnet, alloy for R-T-B rare earth sintered magnet, and method of manufacturing the same
- Patent Title (中): R-T-B系稀土烧结磁体,R-T-B系稀土类烧结磁体用合金及其制造方法
-
Application No.: US14146098Application Date: 2014-01-02
-
Publication No.: US09558872B2Publication Date: 2017-01-31
- Inventor: Takashi Yamazaki , Kenichiro Nakajima
- Applicant: SHOWA DENKO K.K.
- Applicant Address: JP Tokyo
- Assignee: SHOWA DENKO K.K.
- Current Assignee: SHOWA DENKO K.K.
- Current Assignee Address: JP Tokyo
- Agency: Sughrue Mion, PLLC
- Priority: JP2013-000445 20130107; JP2013-256492 20131211
- Main IPC: H01F1/053
- IPC: H01F1/053 ; H01F1/40 ; H01F1/057 ; H01F41/02

Abstract:
An R-T-B rare earth sintered magnet contains R which represents a rare earth element; T which represents a transition metal essentially containing Fe; a metal element M which represents Al and/or Ga; B; Cu; and inevitable impurities the R-T-B rare earth sintered magnet including 13.4 to 17 at % of R, 4.5 to 5.5 at % of B, and 0.1 to 2.0 at % of M, and T as the balance; in which the R-T-B rare earth sintered magnet is formed of a sintered body which includes a main phase composed of R2Fe14B and a grain boundary phase including a larger amount of R than the main phase; in which the magnetization direction of the main phase is a c-axis direction, in which crystal grains of the main phase have one of an elliptical shape and an oval shape extended in such a direction so as to cross the c-axis direction; and in which the grain boundary phase includes an R-rich phase in which the total atomic concentration of the rare earth elements is 70 at % or greater and a transition metal-rich phase in which the total atomic concentration of the rare earth elements is 25 to 35 at %.