Invention Application
- Patent Title: FILLED RESINS AND METHOD FOR MAKING FILLED RESINS
- Patent Title (中): 填充树脂和填充填料的方法
-
Application No.: PCT/US2009038408Application Date: 2009-03-26
-
Publication No.: WO2009120868A3Publication Date: 2009-12-17
- Inventor: NELSON JAMES M , ARCHIBALD MATTHEW N , KOLB BRANT U , THOMPSON WENDY L , SCHULTZ WILLIAM J , HACKETT STEVEN C
- Applicant: 3M INNOVATIVE PROPERTIES CO , NELSON JAMES M , ARCHIBALD MATTHEW N , KOLB BRANT U , THOMPSON WENDY L , SCHULTZ WILLIAM J , HACKETT STEVEN C
- Assignee: 3M INNOVATIVE PROPERTIES CO,NELSON JAMES M,ARCHIBALD MATTHEW N,KOLB BRANT U,THOMPSON WENDY L,SCHULTZ WILLIAM J,HACKETT STEVEN C
- Current Assignee: 3M INNOVATIVE PROPERTIES CO,NELSON JAMES M,ARCHIBALD MATTHEW N,KOLB BRANT U,THOMPSON WENDY L,SCHULTZ WILLIAM J,HACKETT STEVEN C
- Priority: US4032908 2008-03-28
- Main IPC: C08K9/04
- IPC: C08K9/04 ; C08J7/04 ; C08K3/10 ; C08K3/22 ; C08K3/40 ; C08K5/54 ; C08K7/16 ; C08L101/00
Abstract:
A method of making a filled resin includes providing functionalized particles; and combining and homogenously mixing the functionalized particles with an organic matrix in a vacuum kneader to provide the filled resin so that the functionalized particles comprise at least about 20% by weight of the filled resin. The step of providing functionalized particles can also include providing a feedstock of (i) untreated particles, (ii) a surface treatment agent reactive with the particles, and (iii) solvent, and directing the feedstock through a continuous reactor maintained at a temperature sufficient to react the particles with the surface treatment agent to provide the functionalized particles in less than about 4 hours; and directing the functionalized particles from the continuous reactor directly into the vacuum kneader. In another aspect, the a finished resin comprises at least about 20% by weight of functionalized particles in an organic matrix