摘要:
Cellulose acetate propionate is a cellulose ester wherein hydroxyl groups of cellulose are substituted with acetyl and propionyl. Cellulose acetate propionate of the present invention has an amorphous index (Am) of not more than 0.4. Cellulose acetate propionate has a degree of acetyl substitution (DSac) and a degree of propionyl substitution (DSpr), which preferably satisfy the formulas (I) to (III), and more preferably satisfy the formulas (I) to (IV). The present invention also provides a solution of cellulose acetate propionate and a cellulose acetate propionate film. (I) 2.0 (II) 0.05 (III) 2.6 (IV) 1.9
摘要:
A filter rod is produced by adding a water-soluble polymer in the form of an aqueous solution or dispersion, or in a particulate form, to a tow of cellulose ester fiber, with the amount of any water used being controlled within 25 parts by weight relative to 100 parts by weight of the tow, and wrapping the treated tow in wrapping paper. The water contained in the filter rod is removed or the particulate water-soluble polymer is melted by heating to bond the fiber to provide a tobacco filter. The proportion of the water soluble polymer is 0.5 to 30 parts by weight to 100 parts by weight of the tow. To reduce the amount of water relative to the tow, a hot-melt adhesive water-soluble polymer may be employed. As the amount of water added to the tow is thus decreased, the tow can be smoothly wrapped up even at a high speed so that filter productivity is improved. This tobacco filter is highly wet-disintegratable and, hence, contributes to mitigation of the environmental pollution.
摘要:
A filter rod is produced by adding a water-soluble polymer in the form of an aqueous solution or dispersion, or in a particulate form, to a tow of cellulose ester fiber, with the amount of any water used being controlled within 25 parts by weight relative to 100 parts by weight of the tow, and wrapping the treated tow in wrapping paper. The water contained in the filter rod is removed or the particulate water-soluble polymer is melted by heating to bond the fiber to provide a tobacco filter. The proportion of the water soluble polymer is 0.5 to 30 parts by weight to 100 parts by weight of the tow. To reduce the amount of water relative to the tow, a hot-melt adhesive water-soluble polymer may be employed. As the amount of water added to the tow is thus decreased, the tow can be smoothly wrapped up even at a high speed so that filter productivity is improved. This tobacco filter is highly wet-disintegratable and, hence, contributes to mitigation of the environmental pollution.
摘要:
The present invention relates to a film comprising a cellulose triacetate and to a method of producing same. The form of the carboxyl group binding to a cellulose acetate and/or the hemicellulose acetate or the content of an alkali metal or an alkaline earth metal in a cellulose acetate affects releasability and transparency of a film or spinnability of a dope.