公开(公告)号:EP3434468B1
公开(公告)日:2019-07-17
申请号:EP18184953.0
申请日:2018-07-23
申请人: KURARAY CO., LTD.
发明人: ITO, Yu , SUZUKI, Makoto , OKAMOTO, Makoto
-
公开(公告)号:EP3434468A1
公开(公告)日:2019-01-30
申请号:EP18184953.0
申请日:2018-07-23
申请人: KURARAY CO., LTD.
发明人: ITO, Yu , SUZUKI, Makoto , OKAMOTO, Makoto
IPC分类号: B32B7/12 , B32B27/08 , B32B27/18 , B32B27/20 , B32B27/22 , B32B27/30 , B32B27/32 , B32B1/02 , B60K15/03
CPC分类号: B60K15/03 , B32B1/02 , B32B7/12 , B32B27/08 , B32B27/18 , B32B27/20 , B32B27/22 , B32B27/306 , B32B27/32 , B32B2250/03 , B32B2250/246 , B32B2262/101 , B32B2264/102 , B32B2270/00 , B32B2272/00 , B32B2307/30 , B32B2307/308 , B32B2307/558 , B32B2307/7244 , B32B2307/732 , B32B2439/00 , B32B2605/00 , B32B2605/08 , B32B2605/12 , B32B2605/18
摘要: There is provided a fuel container comprising a layer made of a resin composition (E) comprising polyethylene (A), EVOH (B), acid-modified polyethylene (C) and acid-modified polyethylene (D), wherein the resin composition (E) contains 0.1 to 20 parts by mass of EVOH (B), 0.1 to 20 parts by mass of acid-modified polyethylene (C) and 0.1 to 10 parts by mass of acid-modified polyethylene (D) based on 100 parts by mass of polyethylene (A); an MFR (190 °C, under 2.16 kg load) of the polyethylene (A) is 0.01 to 10 g/10 min; an acid value of the acid-modified polyethylene (C) is 0.1 to 9 mg KOH/g; an acid value of the acid-modified polyethylene (D) is more than 10 mg KOH/g and 120 mg KOH/g or less; and a ratio (D/A) of an MFR (190 °C, under 2.16 kg load) of the acid-modified polyethylene (D) to an MFR (190 °C, under 2.16 kg load) of the polyethylene (A) is 50 or more. For a fuel container of the present invention, the amount of deteriorated materials adhering to a screw and/or a die is reduced even when long-term continuous melt molding is conducted during production thereof, resulting in higher productivity. Furthermore, the fuel container exhibits excellent impact resistance with less stripes being generated.
-
公开(公告)号:EP4006101A1
公开(公告)日:2022-06-01
申请号:EP20846637.5
申请日:2020-05-19
申请人: Kuraray Co., Ltd.
发明人: ITO, Yu , OKAMOTO, Makoto , SUZUKI, Makoto
IPC分类号: C08L29/04 , C08L101/00 , C08L101/12 , B29C33/72 , C08K3/00
摘要: A purging agent of the present invention contains a resin composition containing a hydrophilic resin (A), water (B), and a basic compound (C). The mass ratio (A)/(B) of the hydrophilic resin (A) to the water (B) is 66/34 to 90/10, and the content of the basic compound (C) is 0.25 to 7 parts by mass with respect to 100 parts by mass of the hydrophilic resin (A).
-
公开(公告)号:EP3660089A1
公开(公告)日:2020-06-03
申请号:EP18837808.7
申请日:2018-07-23
申请人: Kuraray Co., Ltd.
发明人: ITO, Yu , SUZUKI, Makoto , OKAMOTO, Makoto
摘要: A resin composition (E) includes from 0.1 to 20 parts by mass of an ethylene-vinyl alcohol copolymer (B), from 0.1 to 20 parts by mass of an acid-modified polyolefin (C), and from 0.1 to 10 parts by mass of an acid-modified polyolefin (D) based on 100 parts by mass of a polyolefin (A), wherein the polyolefin (A) has an MFR (190°C, under a load of 2.16 kg) from 0.01 to 10 g/10 min, the acid-modified polyolefin (C) has an acid value from 0.1 to 9 mg KOH/g, the acid-modified polyolefin (D) has an acid value of more than 10 mg KOH/g and 120 mg KOH/g or less, and a ratio (D/A) of an MFR (190°C, under a load of 2.16 kg) of the acid-modified polyolefin (D) to the MFR (190°C, under a load of 2.16 kg) of the polyolefin (A) is 50 or more. The resin composition (E) of the present invention causes reduction in the amount of deteriorated materials adhering to a screw and/or a die even when long-term continuous melt molding is conducted. Use of the resin composition (E) also allows production of a molded article exhibiting excellent impact resistance and appearance. The production method of the present invention allows long-term stable production of the resin composition (E).
-
-
-