摘要:
In quenching , where a heated steel pipe (2) is immersed in a water bath (3) in parallel with water surface for cooling a pipe outer surface, and cooling water is injected from an axial center nozzle (8) into one end of pipe for cooling a pipe inner surface, thereby rapidly cooling the entire pipe surface,, reduction of strength difference along a length of the quenched pipe becomes possible by moving the nozzle (8) following the motion of the pipe axis (2), and starting injecting the water from the nozzle (8) so as for the water to reach the other pipe end at the time of the immersion of the entire circumference of the pipe outer surface. An opening (3a) preferably faces the nozzle (8) to remove the water, and the flow velocity is preferably set to 23 m/sec or more for better water flow inside the pipe (2).
摘要:
A quenching apparatus that can enhance hardenability is provided. A circulation apparatus (50) in the quenching apparatus recovers cooling fluid after the cooling fluid is used for quenching, and supplies the cooling fluid to a defoaming bath (431). A laminar flow weir (433) of a defoaming apparatus (4) partitions the defoaming bath (431) into a laminar flow bath (434) and a shallow bath (435). The laminar flow weir (433) is lower than a side wall of the laminar flow bath (434). Cooling fluid from the circulation apparatus (50) is supplied to the laminar flow bath (434), and the cooling fluid is poured into the shallow bath (435) from the laminar flow bath (434) along the laminar flow weir (433). A filter (432) is a plate shape or a sheet shape and has a mesh structure, and covers an opening in a bottom portion of the shallow bath (435). The liquid level height in the shallow bath (435) is less than the height of the laminar flow weir (433). A supply bath (441) accumulates cooling fluid that passes through the filter (432), and supplies the cooling fluid to a cooling apparatus that sprays the cooling fluid onto a metallic material.
摘要:
A rod or wire manufacturing system, a method for manufacturing a rod or wire, a method for heat treating of a rod' or wire, and a treated metal having an improved tensile strength are disclosed. The cooling unit includes at least one adaptable quenching zone and at least one adaptable soaking zone (isothermal), so as to conduct a patenting treatment. The heat transfer coefficient during quenching and soaking is adjusted by the content of air bubbles in the foamed liquid quenchant, and by the flow velocity thereof. The system can treat a plurality of wires simultaneously.
摘要:
A material to be treated (W) is preheated to a carburising temperature of 750-950°C and is heat-treated in a carburising atmosphere directly supplied with hydrocarbon and oxidizing gases, in which it is heated to 1000-1100°C. Then, the material being treated (W) is forcibly cooled to a temperature below 600°C, the material (W) is reheated to 750-850°C, and then it is hardened by quenching in oil (20), preferably using a laminar flow quenching technique.
摘要:
A process and device are disclosed for quenching workpieces (18). The workpieces (18) are exposed to a flow (26) of quenchant (12). The workpieces (18) and the quenchant (12) are reversibly moved in relation to each other. For that purpose, a first conveyor for the quenchant (12), in particular a pump (44), and a second conveyor, in particular a roller conveyor with transport rollers (16) for the workpieces (18), are designed with reversible transport directions.
摘要:
Beim Abschrecken von Werkstücken, insbesondere zum Härten von Stählen und Stahllegierungen, mittels einer wässrigen Abschreckflüssigkeit, insbesondere mittels einer wässrigen Lösung eines Polymers aus der Gruppe der Polyalkylenglycole (PAG), der modifizierten Polyalkylenglykole, der Polyacrylate (ACR), des Polyvinylpyrrolidons (PVP), durch relatives Eintauchen in einen Abschreckbehälter, wird der Abschreckbehälter außerhalb der Abschreckphase in einen Vorratstank entleert, um das Eindringen von korrosivem Wasserdampf in den Ofen oder seine Vorkammer zu verhindern. Entweder werden die Werkstücke vor dem Fluten des Abschreckbehälters in diesen abgesenkt und die Abschreckflüssigkeit wird anschließend in den Abschreckbehälter gefördert, oder der Abschreckbehälter wird vor dem Absenken der Werkstücke mit der Abschreckflüssigkeit gefüllt , und die Werkstücke werden anschließend in die Abschreckflüssigkeit abgesenkt. Bei einer Vorrichtung zur Durchführung des Verfahrens ist dem Abschreckbehälter (4) mindestens ein Vorratstank (12, 13) mit einer Förderpumpe (16, 22) für die Abschreckflüssigkeit (14, 15) zugeordnet.
摘要:
Es wird ein Verfahren zur Abkühlung erwärmten Materials wie Walzgut durch ein flüssiges Kühlmittel beschrieben, wobei das erwärmte Kühlmittel anschließend unter Nutzung der hierdurch gewonnenen Wärme abgekühlt wird. Hierzu wird das Kühlmittel in einem Kreislauf geführt. Als Kühlmittel wird eine ternäre Pb-Sn-Bi-Legierung verwendet. Eine bevorzugte Vorrichtung zur Durchführung dieses Verfahrens weist ein Abkühlungsbad (2) für das erwärmte Material und ein Erwärmungsbad (3) für die Abkühlung des Kühlmitels auf, wobei beide Bäder hintereinander in den Kreislauf des Kühlmittels eingeschaltet sind. Das Abkühlungsbad dient zweckmäßig zur Kühlung von gewalztem Metall, das vor dem Walzen im Erwärmungsbad erwärmt wurde.
摘要:
A cooling tank for the thermal treatment of the head of rails, whose frame allows obtaining a stable and on average uniform flow of the cooling fluid which touches the head of the immersed rail along the entire tank, with the continuous exchange of the fluid so as to optimize the cooling speed of the head of the rail.