Abstract:
The invention relates to a process for producing superabsorbents, comprising the preparation of partly neutralized acrylic acid by the steps (i) preparing an over-neutralized acrylic acid having a degree of neutralization of at least 100.1 mol-% by mixing of an acrylic acid 1 and a base and (ii) preparing a neutralized acrylic acid having a degree of neutralization from 50 to 85 mol-% by mixing of the over-neutralized acrylic acid and an acrylic acid 2, wherein the content of dimeric acrylic acid in the acrylic acid 2 is lower than the content of dimeric acrylic acid in the acrylic acid 1.
Abstract:
The present invention relates to a process for producing water-absorbent polymer particles by polymerizing droplets of a monomer solution in a surrounding heated gas phase in a reactor comprising a gas distributor (3), a reaction zone (5) and a fluidized bed (27), the gas leaving the reactor is treated in a condenser column (12) with an aqueous solution, the treated gas leaving the condenser column (12) is recycled at least partly to the fluidized bed (27), wherein the gas leaving the condenser column (12) comprises from 0.05 to 0.3 kg steam per kg dry gas and the steam content of the gas entering the gas distributor (3) is less than 80% of the steam content of the gas leaving the condenser column (12).
Abstract:
and an acquisition-distribution layer between having a three dimensional apertured structure having a femal side (5) and a male side (6), wherein the femal side presents a multiplicity of openings extending in the form of through holes in the direction of a lower surface of the same structure being the male side, wherein the quantity of the water absorbent polymer particles within the fluid absorbent core is at least 3 g.
Abstract:
The present invention relates to a process for producing surface-postcrosslinked water-absorbent polymer particles by coating of water-absorbent polymer particles having a content of residual monomers in the range from 0.03 to 15% by weight with at least one surface-postcrosslinker and thermal surface-postcrosslinking at temperatures in the range from 100 to 180° C.