摘要:
A method of producing cement clinker and a second calcined material, wherein the cement clinker is produced in a first production line and the second calcined material is produced from a raw material in a second production line by carrying out the following steps: e) optionally drying the raw material in a dryer, g) calcining the optionally dried raw material in a rotary kiln to obtain the second calcined material, wherein the sensible heat of a hot gas in the first production line is used as a heat source in the calcining step g) for calcining the raw material, and wherein the rotary kiln exhaust gas coming from the calcining step g) is introduced into the first production line for the secondary combustion of the rotary kiln exhaust gas.
摘要:
The invention relates to mortar or concrete produced with a hydraulic binder, comprising aggregates from cinders from the bottom of municipal waste incinerators and/or from slurry from wastewater treatment plants, or other natural or artificial aggregates, of different particle sizes depending of the use thereof as mortar or concrete, and a binder consisting of: glass and/or other pozzolans; pure Portland clinker with gypsum or plaster of Paris, or the resulting cements following the grinding thereof; and/or optionally lime, depending on the quantity of glass and/or pozzolans; all of the materials forming the base of the binder being ground and mixed together until a binder is obtained, together with the aggregates, with cementing mineral neoformations and a strong pozzolanic character.
摘要:
A supplementary cementitious material used in combination with an activator such as Portland cement to produce a hydraulic binder. The supplementary cementitious material is based on physico-chemically treated filter cake product extracted from dredged sediments and can partially replace Portland cement clinker in conventional concrete applications with positive effects on sustainability (reduction of CO2 emissions, upcycling of residues).
摘要:
Method for producing a low-carbon clinker with low energy consumption comprising the following stages: pre-calcination of the limestone present in the raw material, along the pre-calciner and in the cyclone tower; start of the clinkering process with the raw material inlet after pre-calcination, at a temperature higher than 1400°C and with a C 3 S content above 60%; cooling the material, and finally introduction of 5 to 30% of silico-aluminous materials relative to the mass of material which is here processed in the cooling stage, at the cooler head.