Process for producing glass fibre reinforced composites
    52.
    发明公开
    Process for producing glass fibre reinforced composites 审中-公开
    Verfahren zur Herstellung von Glasfaserverbundwerkstoffen

    公开(公告)号:EP2865705A1

    公开(公告)日:2015-04-29

    申请号:EP13190219.9

    申请日:2013-10-25

    摘要: The present invention concerns a process for the production of injection moulded glass fibre reinforced composites from extruded glass fibre reinforced pellets, said process comprising the following steps:
    (A) Providing:
    (a) Glass fibres (2) coated with a silane based sizing composition, said silane based sizing composition comprising at least one sizing reactive moiety, A1, A2, , (b)A thermoplastic matrix polycondensate (2) comprising a first matrix reactive moiety, B1, at a first end of the chain and a second matrix reactive moiety, B2, at a second end of the chain, ,
    (c) A salt (3) selected among an internal lubricant and a nucleating agent comprising a salt reactive moiety, C, capable of reacting with the at least one sizing reactive moiety, A1, A2, and/or with the first or second matrix reactive moiety, B1, B2, said salt reactive moiety, C, being selected among,
    • A metallic cation ,
    • An organic portion having a functionality, f = 1, with a reactive moiety selected among the anionic form of a carboxylic group or a hydroxyl group, and
    • An inorganic anion such as carbonate or sulphate,

    (B) Blending the glass fibres, thermoplastic matrix polycondensate, and salt;
    (C) Forming glass fibre reinforced pellets; and
    (D) Injection moulding a composite part with a composition comprising the reaction product of said glass fibres, thermoplastic matrix polycondesate and salt

    Characterized in that, the salt is added to a blend of thermoplastic matrix composite and glass fibres only after the first and/or second matrix reactive moieties, B1, B2, and the at least one sizing reactive moiety, A1, A2, are given time to react together at least partially.

    摘要翻译: 本发明涉及一种由挤压玻璃纤维增​​强颗粒制备注塑玻璃纤维增​​强复合材料的方法,所述方法包括以下步骤:(A)提供:(a)涂覆有硅烷基施胶组合物的玻璃纤维(2) 所述硅烷基施胶组合物包含至少一种施胶反应性部分A1,A2,(b)在链的第一端包含第一基质反应性部分B1的热塑性基质缩聚物(2)和第二基体反应性 部分,B2,在链的第二端,(c)选自内部润滑剂和成核剂的盐(3),其包含能够与至少一种施胶反应性部分反应的盐反应性部分C, A1,A2和/或与第一或第二基质反应性部分B1,B2,所述盐反应性部分,C选自金属阳离子,有机官能团,f = 1, 其中选择反应性部分 羧基或羟基的阴离子形式,和无机阴离子如碳酸盐或硫酸盐,(B)混合玻璃纤维,热塑性基质缩聚物和盐; (C)玻璃纤维增​​强颗粒的形成; 和(D)用包含所述玻璃纤维,热塑性基质聚蔗糖和盐的反应产物的组合物注塑成型复合部件。其特征在于,仅将盐加入到热塑性基质复合材料和玻璃纤维的共混物中,仅在第一和/ 或第二基质反应性部分B1,B2和至少一个施胶反应性部分A1,A2给予时间至少部分地一起反应。

    COMPOSITION COMPRISING POLYOLS
    56.
    发明公开
    COMPOSITION COMPRISING POLYOLS 审中-公开
    多元醇组成综合

    公开(公告)号:EP2268685A1

    公开(公告)日:2011-01-05

    申请号:EP09721828.3

    申请日:2009-03-18

    摘要: A package for smoking articles comprising an inner shell and an outer shell, the inner shell defining a space for smoking articles and the outer shell defining a cavity to receive the inner shell, the inner and outer shells being hingedly connected such that they pivot relative to each other from a closed position in which the inner shell is received in the outer shell and an open position in which the inner shell extends from the outer shell, wherein the outer shell includes a sidewall that overlaps a sidewall of the inner shell when the inner and outer shells are in their closed position, a recess being formed in the sidewall of one of the inner or outer shells and a tab extending from a corresponding sidewall of the inner or outer shell such that, when the inner and outer shells are in their closed position, the tab locates in said recess.