摘要:
A method for sintering fine iron ore using a dual layer system is disclosed. Two layers of sintering charge are placed on a train of pallets and each of the layers is set on fire at given intervals of time to perform sintering of the charge. The upper layer of the charge is set on fire when the front flame point of the lower layer reaches grates of the pallet. The upper layer may contain, as a solid fuel, coal containing 10 wt% of higher of volatile matter.
摘要:
A method for manufacturing agglomerates of sintered pellets comprises the steps of mixing and pelletizing fine iron ore, flux, binder and return fines, coating pelletized materials, charging the green pellets into a sintering machine (13), drying charged green pellets in a drying furnace (14) and igniting the pellets in an ignition furnace (15), sintering the green pellets in the sintering machine, and measuring a noise level by the use of a noise sensor arranged on a sintering bed and controlling a sintering operation on the basis of the noise level. The noise level during igniting of the green pellets is measured by the use of a noise sensor (20) arranged on an ignition furnace and permeability of the green pellets are controlled on the basis of the noise level. The noise level is measured by the use of plurality of noise sensors (30a, 30b, 30c, 30d) arranged in the longitudinal direction of thesintering machine followed by the ignition furnace and the burn through point is controlled on the basis of the noise level. The noise level is measured by the use of plurality of noise sensors (40) arranged in the direction of a width of apallet following the ignitition furnace and densities of charged materials are controlled on the basis of the measured values.
摘要:
A method for manufacturing agglomerates of fired pellets comprising the steps of: the first pelletization step of adding and mixing fluxes to fine iron ores containing 30 to 95 wt.% of those of 0.125mm or less in particle size to form a mixture and to pelletize the mixture into green pellets; the second pelletization step of adding powder cokes containing 80 to 100 wt.% of those of 1 mm or less in particle size to the green pellets, in amount of 2.5 to 4.0 wt.% to the fine iron ores, to prepare, through pelletization, green pellets coated with the powder cokes; and the sintering step of charging the green pellets coated with the powder cokes into a grate type sintering machine to manufacture the agglomerates of fired pellets. And furthermore, in another method for manufacturing agglomerated of fired pellets, fine iron ores containing 10 to 80 wt.% of those of 0.044mm or less in particle size and powder cokes containing 20 to 70 wt.% of those of 1mm or less in particle size are used.
摘要:
An inclined screen for feeding a raw mix (4) onto a pallet of a sintering apparatus and comprising adjacent bars (2) extending longitudinally of the incline, the bars being axially rotatable by rotating drive means (33, 33a) at their upper ends.
摘要:
A method for manufacturing agglomerates of fired pellets comprising the steps of: the first pelletization step of adding and mixing fluxes to fine iron ores containing 30 to 95 wt.% of those of 0.125mm or less in particle size to form a mixture and to pelletize the mixture into green pellets; the second pelletization step of adding powder cokes containing 80 to 100 wt.% of those of 1 mm or less in particle size to the green pellets, in amount of 2.5 to 4.0 wt.% to the fine iron ores, to prepare, through pelletization, green pellets coated with the powder cokes; and the sintering step of charging the green pellets coated with the powder cokes into a grate type sintering machine to manufacture the agglomerates of fired pellets. And furthermore, in another method for manufacturing agglomerated of fired pellets, fine iron ores containing 10 to 80 wt.% of those of 0.044mm or less in particle size and powder cokes containing 20 to 70 wt.% of those of 1mm or less in particle size are used.
摘要:
The present invention relates to a sintering apparatus comprising a first and a second carbon-comprising thermally conductive substrate arranged at a distance from each other, thereby providing a space for receiving a substrate to be sintered, and provided between a third and a fourth thermally conductive substrate; and heating means for heating the third and/or the fourth thermally conductive substrate at a heating rate of at least 50 °C/s to a temperature between 750 °C and 1400 °C, thereby heating the first and/or the second thermally conductive substrate, respectively, wherein the third and the fourth thermally conductive substrate comprise, independently from one another, one or more metal nitride and/or metal oxide.