METHOD FOR PRODUCING YIELDABLE PAPER AND PLANT FOR IMPLEMENTING THE METHOD
    3.
    发明授权
    METHOD FOR PRODUCING YIELDABLE PAPER AND PLANT FOR IMPLEMENTING THE METHOD 失效
    用于生产的延展性纸和工厂实施该方法

    公开(公告)号:EP0824619B1

    公开(公告)日:2000-02-09

    申请号:EP96910023.9

    申请日:1996-04-04

    IPC分类号: D21F11/00

    CPC分类号: D21F11/00

    摘要: A method for producing yieldable paper, characterised by comprising the following stages: (a) feeding a mix of vegetable fibres to a kneader member (1); (b) mixing the mix with water in the kneader; (c) beating (6) the fibres by rubbing, to obtain a pulp having a degree of beating of at least 30 DEG SR; (d) transferring the beaten pulp into a flow chest (10); (e) feeding the beaten pulp from the flow chest onto a paper web formation cloth (12) with consequent reduction of the water percentage by gravity and vacuum; (f) pressing (14) said web, with consequent further reduction of its water content; (g) initial drying (16) of the preformed paper web to a substantially constant moisture content of between 15 % and 65 %; (h) compacting between pairs of rollers (17), of which one is of hard material comprising surface ribs and driven at greater speed, and the other is of soft material with a smooth surface and driven at lesser speed; (i) final drying (18) to a moisture content of between 15 % and 4 %, preferably 10 %-8 %; (j) glazing (39).

    METHOD FOR PRODUCING YIELDABLE PAPER AND PLANT FOR IMPLEMENTING THE METHOD
    4.
    发明公开
    METHOD FOR PRODUCING YIELDABLE PAPER AND PLANT FOR IMPLEMENTING THE METHOD 失效
    用于生产的延展性纸和工厂实施该方法

    公开(公告)号:EP0824619A1

    公开(公告)日:1998-02-25

    申请号:EP96910023.0

    申请日:1996-04-04

    IPC分类号: D21F11 D21H11 D21H27

    CPC分类号: D21F11/00

    摘要: A method for producing yieldable paper, characterised by comprising the following stages: (a) feeding a mix of vegetable fibres to a kneader member (1); (b) mixing the mix with water in the kneader; (c) beating (6) the fibres by rubbing, to obtain a pulp having a degree of beating of at least 30 °SR; (d) transferring the beaten pulp into a flow chest (10); (e) feeding the beaten pulp from the flow chest onto a paper web formation cloth (12) with consequent reduction of the water percentage by gravity and vacuum; (f) pressing (14) said web, with consequent further reduction of its water content; (g) initial drying (16) of the preformed paper web to a substantially constant moisture content of between 15 % and 65 %; (h) compacting between pairs of rollers (17), of which one is of hard material comprising surface ribs and driven at greater speed, and the other is of soft material with a smooth surface and driven at lesser speed; (i) final drying (18) to a moisture content of between 15 % and 4 %, preferably 10 %-8 %; (j) glazing (39).