Cross-linking of thermosetting resins by means of heating with saturated perfluoropolyether vapour
    4.
    发明公开
    Cross-linking of thermosetting resins by means of heating with saturated perfluoropolyether vapour 失效
    Vernetzung vonhitzehärtbarenHarzen durch Erhitzung mitgesättigtenPerfluorpolyätherdämpfen。

    公开(公告)号:EP0282973A1

    公开(公告)日:1988-09-21

    申请号:EP88104104.0

    申请日:1988-03-15

    申请人: AUSIMONT S.r.l.

    IPC分类号: C08J3/24

    CPC分类号: C08J3/247

    摘要: The cross-linking or curing of thermosetting resins and of hot curable elastomers is carried out by heating the mate­rial or the article comprising the resin (or the elastomer) by means of saturated vapour of a commercial perfluoropolye­ther having an average boiling point corresponding to the temperature necessary for the cross-linking and having a boil­ing point range not exceeding 12°C (measured according to ASTM D 1078) in the presence of a chlorofluorohydrocarbon seconda­ry vapour.

    摘要翻译: 热固性树脂和热固化弹性体的交联或固化通过用平均沸点对应于温度的商业全氟聚醚的饱和蒸气加热材料或包含树脂(或弹性体)的物品来进行 在氯氟烃二次蒸气的存在下,交联必要且沸点范围不超过12℃(根据ASTM D 1078测量)。