摘要:
An object of the invention of the present application is to provide an adhesive composition excellent in tackiness, tack strength, retentivity and coating property. The adhesive composition according to the invention of the present application contains a block copolymer (a) having a block mainly comprising a vinyl aromatic monomer unit, a tackifier (b) and an oil (c), in which the block copolymer (a) contains a partially hydrogenated block copolymer (a-1), the partially hydrogenated block copolymer (a-1) has a vinyl aromatic monomer unit and a conjugated diene monomer unit, the content of the vinyl aromatic monomer unit is 10 mass% or more and 19 mass% or less based on 100 mass% of the partially hydrogenated block copolymer (a-1), and the hydrogenation ratio of double bonds contained in the conjugated diene monomer unit in the partially hydrogenated block copolymer (a-1) is 15 mol% or more and less than 80 mol% based on the total (amount) of double bonds before hydrogenation.
摘要:
A partially hydrogenated block copolymer of the present invention includes: a polymer block (A) containing a vinyl aromatic monomer unit as a main component: and a polymer block (B) containing a conjugated diene monomer unit, wherein in a differential molecular weight distribution (B) of a degradation product of the partially hydrogenated block copolymer obtained by an ozone degradation method, a distribution of degree of hydrogenation H, which is given by a maximum peak height in a region of a molecular weight of 800 or more and 3,000 or less, is 0.01 to 0.5.
摘要:
A block copolymer composition including: 10% by mass or more and 90% by mass or less of a component (a), and 10% by mass or more and 90% by mass or less of a component (b), wherein the component (a) is a block copolymer containing a polymer block (A) primarily including a vinyl aromatic monomer unit and a polymer block (B) primarily including a conjugated diene monomer unit, wherein the block copolymer has a weight average molecular weight of 30,000 or higher and 150,000 or lower; the component (b) is a block copolymer containing a polymer block (A) primarily including a vinyl aromatic monomer unit and a polymer block (B) primarily including a conjugated diene monomer unit; the component (b) includes a component (b-2) at a ratio of weight average molecular weight to the weight average molecular weight of the component (a) of 2.5 or more and less than 3.4, and a component (b-3) at a ratio of weight average molecular weight to the weight average molecular weight of the component (a) of 3.4 or more and less than 4.5; and the content of the vinyl aromatic monomer unit in the component (a) and the component (b) is 10 to 50% by mass based on the total amount of the component (a) and the component (b).
摘要:
A water-developable plate package comprising water-developable plates packaged in a laminated state. The water developable plate is a sheet-like plate comprising a photosensitive layer made of a photosensitive resin composition having water-developability and a protective film covering both surfaces of this photosensitive layer. The package prevents the occurrence of deformation of the plates in a packaged state during transportation or storage at a high temperature and a high humidity in summer without complicating the operations at the time of use or packaging of plates and without increasing the cost remarkably. The package is obtained by sandwiching an open-cell foam sheet (2) between the water-developable plates (1 and 1) to form a laminate (3), wrapping the laminate (3) with a light-screening film and fixing the wrapping ends with a tape. Because the foam sheet (2) exists, in-plane non-uniformity of hygroscopicity of the plates (1) can be corrected during transportation or storage at a high temperature and high humidity in summer, and the deformation of the plates (1) can be restricted.
摘要:
A block copolymer (P) that is a hydrogenated product of a block copolymer comprising a polymer block (A) mainly composed of a vinyl aromatic monomer unit and a polymer block (B) mainly composed of a conjugated diene monomer unit, the block copolymer (P) satisfying the following conditions (1) and (2): (1) a 5% by mass toluene solution viscosity at 25°C is 5 mPa·s or more and 45 mPa·s or less (2) the block copolymer (P) comprises a functional group.
摘要:
The present invention provides a molded bale of a rubber-like block copolymer, satisfying the following requirements 1 to 6: Requirement 1: a content of a vinyl aromatic monomer unit is 9% by mass or more and 50% by mass or less; Requirement 2: a proportion of a vinyl aromatic monomer block is 3% by mass or more and less than 30% by mass; Requirement 3: an iodine value is 3 to 250; Requirement 4: a proportion of an ethylene structure is 3% by mass or more; Requirement 5: a weight average molecular weight is in a range of 80,000 to 1,000,000; and Requirement 6: at least one block at a molecular end is a specific block I or block II.
摘要:
A hydrogenated conjugated diene-based polymer of the present invention has a branch number (Bn) measured by viscosity detector-equipped GPC-light scattering measurement of 2.5 or more, and a hydrogenation rate of a structural unit derived from a conjugated diene compound of 30% or more and less than 99%.
摘要:
A production method for a branched conjugated diene-based polymer, comprising: a polymerizing step of obtaining a conjugated diene-based polymer having an active end by polymerizing or copolymerizing a conjugated diene compound, or a conjugated diene compound and an aromatic vinyl compound with an alkali metal compound or an alkaline earth metal compound used as a polymerization initiator; and a branching step of introducing a branch structure by reacting a styrene derivative as a branching agent with the active end of the conjugated diene-based polymer.
摘要:
A thermoplastic resin composition comprising: a block copolymer (a) having 60 to 80% by mass of a vinyl aromatic monomer unit and 40 to 20% by mass of a conjugated diene monomer unit; and a copolymer (b) having 60 to 90% by mass of a vinyl aromatic monomer unit and 40 to 10% by mass of an unsaturated nitrile monomer unit, wherein the block copolymer (a) has at least one polymer block (S) primarily having a vinyl aromatic monomer unit, the block copolymer (a) has at least one tan ´ peak of dynamic viscoelasticity at a temperature in a range of -73 to -10°C, and a mass ratio (a)/(b) of the block copolymer (a) to the copolymer (b) is 1/99 to 80/20.