摘要: A polyolefin nanocomposite material comprising the following components: (A) a crystalline or semi-crystalline polyolefin resin; and (B) a nanosized mineral filler comprising or substantially consisting of a hydrotalcite, wherein the amount of the hydrotalcite is from 0.02 to 6 parts by weight per 100 parts by weight of the nanocomposite material, and the ratio MFR (1)/MFR (2) of the melt flow rate value MFR (1) of component (A) to the melt flow rate value MFR (2) of the polyolefin nanocomposite material is of at least 1.02, characterized in that the said polyolefin nanocomposite material includes a compatibilizer the dispersion of the mineral filler (B) and compatibilizer in the polyolefin resin is produced at shear mixing rates from 30 to 300 sec−1,
摘要翻译: 一种聚烯烃纳米复合材料,其包含以下组分:(A)结晶或半结晶聚烯烃树脂; 和(B)包含或基本上由水滑石组成的纳米尺寸矿物填料,其中所述水滑石的量为每100重量份纳米复合材料0.02至6重量份,并且MFR(1)/ MFR 组分(A)的熔体流动速率值MFR(1)与聚烯烃纳米复合材料的熔体流动速率值MFR(2)的比值(2)为至少1.02,其特征在于所述聚烯烃纳米复合材料包括增容剂 矿物填料(B)和增容剂在聚烯烃树脂中的分散是以剪切速率为30-300秒-1,
-
公开(公告)号:EP1893685A1
公开(公告)日:2008-03-05
申请号:EP06763296.8
申请日:2006-05-26
CPC分类号: C08L23/02 , B82Y30/00 , C08J5/005 , C08J2323/02 , C08K3/346 , C08K9/04 , C08L23/10 , C08L23/12 , C08L51/06 , C08L2203/12 , C08L2205/08 , D01F1/10 , D01F6/04 , Y10T428/259 , Y10T428/2913 , Y10T442/60 , C08L2666/24
摘要: A polyolefin nanocomposite material comprising the following components: (A) a crystalline or semi-crystalline polyolefin resin; and (B) a nanosize layered mineral filler, wherein the amount of inorganic fraction of the layer mineral filler is from 0.02 to 3 parts by weight per 100 parts by weight of polyolefin resin (A), and the ratio MFR (1)/MFR (2) of the melt flow rate value MFR (1) of component (A) to the melt flow rate value MFR (2) of the polyolefin nanocomposite material is of at least 1.02
摘要翻译: 一种聚烯烃纳米复合材料,其包含以下组分:(A)结晶或半结晶聚烯烃树脂; 和(B)纳米级层状矿物填料,其中层状矿物填料的无机部分的量为每100重量份聚烯烃树脂(A)0.02-3重量份,MFR(1)/ MFR (A)的熔体流动速率值MFR(1)与聚烯烃纳米复合材料的熔体流动速率值MFR(2)的比(2)为至少1.02
-
公开(公告)号:EP2215155A2
公开(公告)日:2010-08-11
申请号:EP08855521.4
申请日:2008-10-15
CPC分类号: C08K3/26 , C08L23/20 , C08L51/06 , Y10T428/139 , Y10T442/60 , C08L23/02 , C08L2666/24
摘要: A polyolefin nanocomposite material comprising the following components: (A) a crystalline or semi-crystalline polyolefin resin; and (B) a nanosized mineral filler comprising or substantially consisting of a hydrotalcite, wherein the amount of the hydrotalcite is from 0.02 to 6 parts by weight per 100 parts by weight of the nanocomposite material, and the ratio MFR (1)/MFR (2) of the melt flow rate value MFR (1) of component (A) to the melt flow rate value MFR (2) of the polyolefin nanocomposite material is of at least 1.02, characterized in that the said polyolefin nanocomposite material includes a compatibilizer the dispersion of the mineral filler (B) and compatibilizer in the polyolefin resin is produced at shear mixing rates from 30 to 300 sec−1,
-
-