公开(公告)号:EP2994256B1
公开(公告)日:2019-03-27
申请号:EP14834940.0
申请日:2014-04-30
申请人: Borgwarner Inc.
IPC分类号: B22D18/02
-
公开(公告)号:EP2994256A2
公开(公告)日:2016-03-16
申请号:EP14834940.0
申请日:2014-04-30
申请人: Borgwarner Inc.
IPC分类号: B22D18/02
CPC分类号: B22D18/02 , B22D21/005
摘要: A process for casting TiAl components, having the following process steps: producing a melt (S) of the TiAl material below an inert gas fill (IF); placing a casting mold (1) on a gate (2) in a gastight manner; flooding the casting mold (1) with inert gas (IG) by opening a closure mechanism (7) which is arranged at the gate (2) and is connected to an inert gas source (8); pressing the melt (S) through the gate (2) into the casting mold (1) by increasing the pressure (P) of the inert gas fill (IF) above the melt (S) while at the same time evacuating the inert gas (IG) from the casting mold (1), and stopping the inflow of inert gas (IG) as soon as it is determined that the melt (S) passes above the position of the closure mechanism (7).
摘要翻译: 本发明涉及一种用于铸造TiAl成分的方法,其包括以下工艺步骤:在惰性气体填充(IF)下方产生TiAl材料的熔体(S); 将浇铸模具(1)以气密方式放置在浇口(2)上; 通过打开布置在所述门(2)处并连接到惰性气体源(8)的关闭机构(7),用惰性气体(IG)充注所述铸模(1); 通过增加熔体(S)上方的惰性气体填充物(IF)的压力(P),同时抽空惰性气体((S)),将熔体(S)通过浇口(2)压入铸模(1) IG)从铸模(1)流出,并且一旦确定熔体(S)经过关闭机构(7)的位置之上,就立即停止惰性气体(IG)的流入。
-
-
公开(公告)号:EP3535480A1
公开(公告)日:2019-09-11
申请号:EP17804693.4
申请日:2017-10-31
申请人: Borgwarner Inc.
IPC分类号: F01D25/24
-
-
-