METHOD FOR MANUFACTURING SURFACE-MODIFIED MOLDED ARTICLE, AND METHOD FOR MANUFACTURING COMPOSITE USING SURFACE-MODIFIED MOLDED ARTICLE
    2.
    发明公开
    METHOD FOR MANUFACTURING SURFACE-MODIFIED MOLDED ARTICLE, AND METHOD FOR MANUFACTURING COMPOSITE USING SURFACE-MODIFIED MOLDED ARTICLE 审中-公开
    制造表面改性模制制品的方法以及使用表面改性模制制品制造复合材料的方法

    公开(公告)号:EP3190148A1

    公开(公告)日:2017-07-12

    申请号:EP15837867.9

    申请日:2015-09-04

    申请人: Osaka University

    IPC分类号: C08J7/00 B32B27/30 C08J5/12

    摘要: An object of the present invention is to provide a process for producing a surface-modified molded article, whereby surface layer strength of a molded article can be enhanced, and a molded article containing an organic polymer compound with low adhesive property, such as a fluororesin, can be bonded to an adherend without the use of an adhesive, and whereby a treatment step or an apparatus in an atmospheric-pressure plasma treatment are not complicated, and to provide a process for producing a composite of the surface-modified molded article and an adherend. The present invention is a process for producing a surface-modified molded article wherein a surface of the molded article containing an organic polymer compound is subjected to an atmospheric pressure plasma treatment to introduce a peroxide radical with adjusting the surface temperature of the molded article to (melting point of the organic polymer compound - 120)°C or higher.

    摘要翻译: 本发明的目的在于提供可提高成型品的表层强度的表面改性成型品的制造方法,以及含有氟树脂等粘接性低的有机高分子化合物的成型品 可以在不使用粘合剂的情况下粘合至被粘物,并且由此常压等离子体处理中的处理步骤或设备不复杂,并且提供用于制备表面改性的模塑制品和 一名被害人。 本发明是一种生产表面改性模塑制品的方法,其中将含有有机高分子化合物的模塑制品的表面进行常压等离子体处理以引入过氧化物自由基,并将模塑制品的表面温度调节至( 有机高分子化合物的熔点-120℃)以上。

    METHOD AND APPARATUS FOR SURFACE TREATING FLUORORESIN FILM

    公开(公告)号:EP3406658A1

    公开(公告)日:2018-11-28

    申请号:EP16886430.4

    申请日:2016-11-04

    IPC分类号: C08J7/00 H05H1/46 H05K3/38

    CPC分类号: C08J7/00 H05H1/46 H05K3/38

    摘要: It is an objective of the present invention to improve coatability/printability and adhesiveness of a fluorine-based resin film to a sintered film of ink. A fluorine-based resin film 9 is passed through a treatment space 1a under near atmospheric pressure between electrodes 11, 21. A process gas composed of an inert gas is supplied to the treatment space 1a. Voltage is applied to between the electrodes to generate electric discharge in the treatment space 1a. A treatment surface 9a is heated to a temperature that is not higher than a continuous use temperature and not lower than a temperature lower than the continuous use temperature by 100 degrees C. A volume concentration of oxygen in the treatment space 1a is not higher than 1000 ppm.