公开(公告)号:EP1100596A1
公开(公告)日:2001-05-23
申请号:EP00923340.4
申请日:2000-04-14
CPC分类号: B29C70/70 , A63B37/0003 , A63B37/0052 , A63B37/0056 , A63B37/0064 , A63B37/0065 , A63B37/0067 , A63B37/0075 , A63B37/0076 , A63B45/00 , B29C2045/14877 , B29L2031/54 , B29L2031/545 , Y10S264/65
摘要: A method of manufacturing golf balls (25) that prevents the cover (22) from cracking due to thermal expansion of the core (20) during the cover (22) formation process is disclosed herein. The method includes the forming a core (20), with one or more optional boundary layers (21), and then pre-heating the core (20) and any boundary layer (21) to generate volumetric thermal expansion thereof. After the pre-heating, the cover (22) of the golf ball (25) is formed over the core (20) and any boundary layer (21). The method of the present invention also decreases cover (22) molding cycle time for golf balls (25).