摘要:
A cigarette filter material useful for selectively and efficiently reducing formaldehyde while maintaining a palatable component such as nicotine or tar is provided. A cigarette filter material is obtained by adhesively treating a substrate (such as a cellulose acetate fiber) with a dispersion comprising a particulate polysaccharide having an amino group (e.g., chitosan) and a medium. The medium may be a polar solvent (e.g., water, and an alcohol), and a plasticizer for the substrate. A cigarette filter comprising such cigarette filter material can efficiently and selectively reduce formaldehyde. For example, the cigarette filter ensures a retention of formaldehyde of not more than 65% while maintaining retentions of nicotine and tar of not less than 75%, respectively.
摘要:
An object of the invention is to obtain cellulose acetate with improved physical properties, particularly film strength and improved flexibility of the molded product. Cellulose acetate wherein average degree of acetylation is not less than 59 %, viscosity average degree of polymerization (DP) is not less than 290, and concentrated solution viscosity (η) according to falling ball viscosity method for viscosity average degree of polymerization (DP) is expressed by the following formula (1): 2.814 × ln(DP) - 11.753 ≦ ln(η) ≦ 7.28 × ln(DP) - 37.059 and a process for production thereof.
摘要:
The present invention provides a cellulose acetate satisfying at least one requirement selected from the following requirements (A) , (B) and (C), provided that the case where (B) alone is satisfied is excluded.
Requirement (A) : Bright spotty matters in sizes of 20 µm or more are not more than 20 units/mm 3 . Requirement (B) : Blocking constant (K) is not more than 60. Requirement (C): The ratio (G'/G") of storage modulus (G') to loss modulus (G") at a measuring frequency of 0.016Hz is not more than 0.2.
摘要翻译:本发明提供满足以下要求(A),(B)和(C)中至少一个要求的乙酸纤维素乙酸酯,只要满足(B)单独满足的情况即可。 要求(A):尺寸为20亩以上的亮点不大于20单位/ mm 3。 要求(B):阻塞常数(K)不大于60.要求(C):测量频率为0.016时储能模量(G')与损耗模量(G“)的比值(G'/ G”) Hz不大于0.2。
摘要:
Cellulose acetate of high moldability with low solution viscosity in spite of high average degree of polymerization is obtained. Low molecular weight components of cellulose acetate (e.g., CTA having average degree of acetylation of 59.0 to 62.5 %) are eluted with a washing solvent to produce cellulose acetate having molecular weight distribution Mw/Mn of 1 to 1.7. As washing solvent, those swell or partially dissolve cellulose acetate, for example, those dissolve 0.1 to 30 % by weight of cellulose acetate can be used. Such solvent includes, for example, a solvent having solubility parameter δ of 7 to 12.5 (ketones, ethers, organic acid, esters, etc.).