    摘要: In a process for producing a reduction gas containing hot CO and H2 for reducing lump ore, particularly iron ore, the reduction gas is formed by gasification of carbon containing materials, particularly coal, under the addition of oxygen in a gasification zone (8) and subsequently cooled to a reduction gas temperature conducive to the reduction process. To produce a reduction gas of greater thermodynamic stability, H2O and/or CO2 are added to eliminate the Boudouard and heterogeneous water gas reaction and the concomitant warming of the reduction gas.

    摘要翻译: 在用于还原块状矿石,特别是铁矿石的含有热CO和H 2的还原气体的过程中,还原气体是通过在气化区(8)中加入氧气气化含碳物质,特别是煤气而形成的,和 随后冷却至有利于还原过程的还原气体温度。 为了产生热力学稳定性更高的还原气体,加入H 2 O和/或CO 2以消除Boudouard和非均相水煤气反应以及伴随的还原气体的升温。