摘要:
The present invention provides a hot-forgeable Ni-based superalloy excellent in high temperature strength, including, in terms of % by mass: C: more than 0.001% and less than 0.100%, Cr: 11.0% or more and less than 19.0%, Co: 0.5% or more and less than 22.0%, Fe: 0.5% or more and less than 10.0%, Si: less than 0.1%, Mo: more than 2.0% and less than 5.0%, W: more than 1.0% and less than 5.0%, Mo+1/2W: 2.5% or more and less than 5.5%, S: 0.010% or less, Nb: 0.3% or more and less than 2.0%, Al: more than 3.00% and less than 6.50%, and Ti: 0.20% or more and less than 2.49%, with the balance being Ni and unavoidable impurities, in which (Ti/Al)×10 is 0.2 or more and less than 4.0 in terms of atomic ratio, and in which Al+Ti+Nb is 8.5% or more and less than 13.0% in terms of atomic%.
摘要:
Provided is a maraging steel excellent in fatigue characteristics, including, in terms of % by mass: C: ≤0.015%, Ni: from 12.0 to 20.0%, Mo: from 3.0 to 6.0%, Co: from 5.0 to 13.0%, Al: from 0.01 to 0.3%, Ti: from 0.2 to 2.0%, O: ≤0.0020%, N: ≤0.0020%, and Zr: from 0.001 to 0.02%, with the balance being Fe and unavoidable impurities.
摘要:
The present invention relates to an Ni-based superalloy for hot forging, containing, in terms of % by mass, C: more than 0.001 % and less than 0.100%, Cr: 11% or more and less than 19%, Co: more than 5% and less than 25%, Fe: 0.1% or more and less than 4.0%, Mo: more than 2.0% and less than 5.0%, W: more than 1.0% and less than 5.0%, Nb: 2.0% or more and less than 4.0%, Al: more than 3.0% and less than 5.0%, and Ti: more than 1.0% and less than 3.0%, with the balance being unavoidable impurities and Ni, in which the component composition satisfies the following two relationships: 3.5 ≤ ([Ti]+[Nb])/[Al]×10
摘要:
The present invention provides a hot-forgeable Ni-based superalloy excellent in high temperature strength, including, in terms of % by mass: C: more than 0.001% and less than 0.100%, Cr: 11.0% or more and less than 19.0%, Co: 0.5% or more and less than 22.0%, Fe: 0.5% or more and less than 10.0%, Si: less than 0.1%, Mo: more than 2.0% and less than 5.0%, W: more than 1.0% and less than 5.0%, Mo+1/2W: 2.5% or more and less than 5.5%, S: 0.010% or less, Nb: 0.3% or more and less than 2.0%, Al: more than 3.00% and less than 6.50%, and Ti: 0.20% or more and less than 2.49%, with the balance being Ni and unavoidable impurities, in which (Ti/Al)×10 is 0.2 or more and less than 4.0 in terms of atomic ratio, and in which Al+Ti+Nb is 8.5% or more and less than 13.0% in terms of atomic%.
摘要:
The present invention relates to an Ni-based superalloy for hot forging, containing, in terms of % by mass, C: more than 0.001 % and less than 0.100%, Cr: 11% or more and less than 19%, Co: more than 5% and less than 25%, Fe: 0.1% or more and less than 4.0%, Mo: more than 2.0% and less than 5.0%, W: more than 1.0% and less than 5.0%, Nb: 2.0% or more and less than 4.0%, Al: more than 3.0% and less than 5.0%, and Ti: more than 1.0% and less than 3.0%, with the balance being unavoidable impurities and Ni, in which the component composition satisfies the following two relationships: 3.5 ‰¤ ([Ti]+[Nb])/[Al]×10
摘要:
Provided is a precipitation hardened Fe-Ni alloy having the following constitutions: (1) the precipitation hardened Fe-Ni alloy including: from 0.01 to 0.08% by mass of C, from 0.02 to 1.0% by mass of Si, not more than 1.0% by mass of Mn, from 36.0 to 41.0% by mass of Ni, 14.0 or more and less than 20.0% by mass of Cr, from 0.01 to 3.0% by mass of Mo, from 0.1 to 1.0% by mass of Al, from 1.0 to 2.5% by mass of Ti, and from 2.0 to 3.5% by mass of Nb, with the balance being Fe and unavoidable impurities; (2) the precipitation hardened Fe-Ni alloy satisfying the following formulae: Ni≥6×Nb+17 and Nb/(Ti+Al)0.8.
摘要:
The present invention provides a maraging steel containing: 0.10≤C≤0.30 mass%, 6.0≤Ni≤9.4 mass%, 11.0≤Co≤20.0 mass%, 1.0≤Mo≤6.0 mass%, 2.0≤Cr≤6.0 mass%, 0.5≤Al≤1.3 mass%, and Ti≤0.1 mass%, with the balance being Fe and unavoidable impurities, and satisfying 1.00≤A≤1.08, in which A is 0.95+0.35×[C]-0.0092×[Ni]+0.011×[Co]-0.02[Cr]-0.001×[Mo], where [C] indicates a content (mass%) of C, [Ni] indicates a content (mass%) of Ni, [Co] indicates a content (mass%) of Co, [Cr] indicates a content (mass%) of Cr, and [Mo] indicates a content (mass%) of Mo, respectively. The maraging steel has a tensile strength of 2,300 MPa or more and is also excellent in the toughness/ductility and fatigue characteristics.
摘要:
The present invention provides a hot-forgeable Ni-based superalloy excellent in high temperature strength, including, in terms of % by mass: C: more than 0.001% and less than 0.100%, Cr: 11.0% or more and less than 19.0%, Co: 0.5% or more and less than 22.0%, Fe: 0.5% or more and less than 10.0%, Si: less than 0.1%, Mo: more than 2.0% and less than 5.0%, W: more than 1.0% and less than 5.0%, Mo+1/2W: 2.5% or more and less than 5.5%, S: 0.010% or less, Nb: 0.3% or more and less than 2.0%, Al: more than 3.00% and less than 6.50%, and Ti: 0.20% or more and less than 2.49%, with the balance being Ni and unavoidable impurities, in which (Ti/Al)×10 is 0.2 or more and less than 4.0 in terms of atomic ratio, and in which Al+Ti+Nb is 8.5% or more and less than 13.0% in terms of atomic%.