公开(公告)号:EP3044364B1
公开(公告)日:2017-11-22
申请号:EP14777538.1
申请日:2014-09-08
发明人: SCHULTE, Johann , HÜPPERLING, Frank , DÖRK, Markus
-
公开(公告)号:EP3044364A1
公开(公告)日:2016-07-20
申请号:EP14777538.1
申请日:2014-09-08
发明人: SCHULTE, Johann , HÜPPERLING, Frank , DÖRK, Markus
CPC分类号: D21H17/37 , D21C3/02 , D21C3/20 , D21C3/222 , D21H17/375 , D21H17/64 , D21H17/65 , D21H17/70 , D21H21/10
摘要: The invention relates to a method for producing paper with at least one fibrous material, a polymer, water and calcium oxide and/or calcium hydroxide, comprising the steps of disintegrating the fibrous material with water in a pulper for producing a fibrous material suspension and transferring the fibrous material suspension into a vat. The method is characterised in that in the disintegration of the fibrous material in the pulper calcium oxide and/or calcium hydroxide having a proportion of active substance between 0.1 kg per tonne of oven-dry fibrous material and 50 kg per tonne of fibrous material for setting of a pH value between 9 and 12 is added to the fibrous material suspension, and in the vat an acrylamide copolymer having a proportion of active substance between 0.1 kg per tonne of oven-dry fibrous material and 10 kg per tonne of fibrous material is added.
摘要翻译: 本发明涉及一种生产具有至少一种纤维材料,聚合物,水和氧化钙和/或氢氧化钙的纸的方法,包括以下步骤:在碎浆机中用水分解纤维材料以产生纤维材料悬浮液和转移 将纤维材料悬浮于大桶中。 该方法的特征在于,在碎浆机中的纤维材料的分解中,一氧化钙和/或氢氧化钙的活性物质比例为0.1kg /烘干纤维材料,每吨纤维材料为50kg,用于固化 在纤维材料悬浮液中加入pH值介于9和12之间,在桶中加入活性物质比例为0.1kg /烘干纤维材料和10kg /吨纤维材料的丙烯酰胺共聚物 。
-