ETHYLENE-BASED POLYMER COMPOSITIONS FOR IMPROVED EXTRUSION COATINGS
    4.
    发明公开
    ETHYLENE-BASED POLYMER COMPOSITIONS FOR IMPROVED EXTRUSION COATINGS 审中-公开
    基于乙烯的聚合物组合物用于改进的挤出涂层

    公开(公告)号:EP3317348A1

    公开(公告)日:2018-05-09

    申请号:EP15744758.2

    申请日:2015-06-30

    IPC分类号: C08L23/06 C09D123/06

    摘要: The invention provides a composition comprising at least the following: a) a first composition comprising at least one first ethylene-based polymer, formed by high pressure, free-radical polymerization, and wherein the first composition comprises the following properties: a melt index (I2) from 1.0 to 15.0 g/10 min, and density from 0.910 to 0.940 g/cc; b) a second composition comprising at least one second ethylene-based polymer, and wherein the second composition comprises the following properties; a melt index (I2) from 1.0 to 1000 g/10 min, a density greater than 0.940 g/cc; wherein the composition comprises the following properties: melt index (I2) from 2.0 to 20.0 g/10 min, and a density from 0.915 to 0.940 g/cc; and wherein the first composition is present in an amount from 65 to 95 wt %, based on the weight of the composition.

    PROCESS TO PREPARE ETHYLENE-BASED POLYMERS USING A DISTRIBUTION OF CARBON MONOXIDE
    6.
    发明公开
    PROCESS TO PREPARE ETHYLENE-BASED POLYMERS USING A DISTRIBUTION OF CARBON MONOXIDE 审中-公开
    工艺生产乙烯基聚合物使用一氧化碳的分布

    公开(公告)号:EP3161024A1

    公开(公告)日:2017-05-03

    申请号:EP15742146.2

    申请日:2015-06-24

    IPC分类号: C08F210/18 C08G67/02 C08F2/34

    摘要: The invention provides a high pressure, free-radical polymerization process for polymerizing an ethylene-based polymer, said process comprising polymerizing ethylene, in a reactor configuration comprising a reactor with at least two reaction zones, a first reaction zone and a reaction zone located downstream from the first reaction zone; and wherein CO (carbon monoxide) is added to the reactor in at least one reaction zone located downstream from the first reaction zone, and wherein, less than, or equal to, 95 weight percent of the total amount of CO, is fed to the first reaction zone.

    摘要翻译: 本发明提供一种高压,自由基聚合方法用于在基于乙烯的聚合物聚合,所述方法包括聚合乙烯在反应器构造包括反应器具有至少两个反应区,第一反应区和位于下游的反应区 从所述第一反应区; 和worin CO(一氧化碳)被添加到反应器中95重量%的CO的总量的位于下游的第一反应区的至少一个反应区,和worin,小于或等于,被供给到 第一反应区。

    ETHYLENE-BASED POLYMERS AND PROCESSES TO MAKE THE SAME
    9.
    发明公开
    ETHYLENE-BASED POLYMERS AND PROCESSES TO MAKE THE SAME 审中-公开
    乙烯基聚合物VERFAHREN ZUR HERSTELLUNG DAVON

    公开(公告)号:EP2900704A1

    公开(公告)日:2015-08-05

    申请号:EP13716496.8

    申请日:2013-03-13

    IPC分类号: C08F10/02

    摘要: An ethylene-based polymer, which is a low density polyethylene (LDPE), obtained by free radical polymerization of ethylene, and wherein the LDPE has a GPC parameter “LSP” less than 1.60. An ethylene-based polymer that comprises the following features: a) at least 0.1 amyl groups per 1000 total carbon atoms; b) a melt index of 0.01 to 0.3; c) a z-average molecular weight of Mz (conv.) of greater than 350,000 g/mol and less than 425,000 g/mol; d) a gpcBR value from 1.50 to 2.05, and e) a MWD(conv) [Mw(conv)/Mn(conv)] from 6 to 9. An ethylene-based polymer that comprises the following features: a) at least 0.1 amyl groups per 1000 total carbon atoms; b) a melt viscosity ratio (V0.1/V100), at 190° C., greater than, or equal to, 58; c) a melt viscosity at 0.1 rad/s, 190° C., greater than, or equal to, 40,000 Pa·s, and d) a gpcBR value from 1.50 to 2.25.

    摘要翻译: 通过乙烯的自由基聚合获得的低密度聚乙烯(LDPE)的乙烯类聚合物,其中LDPE具有小于1.60的GPC参数“LSP”。 一种乙烯基聚合物,其包含以下特征:a)每1000个总碳原子至少0.1个戊基; b)熔体指数为0.01〜0.3; c)Mz(转化)的Z-平均分子量大于350,000g / mol且小于425,000g / mol; d)gpcBR值为1.50至2.05,e)MWD(conv)[Mw(conv)/ Mn(conv)]为6至9.一种乙烯基聚合物,其包含以下特征:a)至少0.1 每1000个总碳原子的戊基; b)熔体粘度比(V0.1 / V100),在190℃,大于或等于58; c)0.1rad / s,190℃,大于或等于40,000Pa·s的熔体粘度,和d)gpcBR值为1.50-2.25。