摘要: The present invention concerns a process for making a polyareneazole multifilament yarn comprising: a) extruding a solution comprising polyareneazole polymer and polyphosphoric acid through a plurality of orifices to produce filaments; b) forming a multifilament yarn from said filaments; c) hydrolyzing at least some of the polyphosphoric acid in the yarn by heating the yarn to a temperature above about 120 0C for up to about two minutes; d) washing at least some of the hydrolyzed polyphosphoric acid from the yarn; e) drying the washed yarn; f) optionally, heating the yarn above about 300 0C, and g) collecting the yarn at a speed of at least about 50 meters per minute.
摘要翻译: 本发明涉及一种制备聚芳烃唑复丝纱的方法,该方法包括:a)将包含聚芳唑聚合物和聚磷酸的溶液通过多个孔挤出以生产长丝; b)由所述长丝形成复丝纱线; c)通过将纱线加热至约120℃以上的温度至多约2分钟来水解纱线中的至少一些多磷酸; d)从纱线中洗涤至少一些水解的多聚磷酸; e)将洗过的纱线干燥; f)可选地,将纱线加热至约300℃以上,并且g)以至少约50米/分钟的速度收集纱线。
-
公开(公告)号:EP1877466B1
公开(公告)日:2014-02-26
申请号:EP06739679.6
申请日:2006-03-27
发明人: ALLEN, Steven, R. , MOORE, Stephen, D. , NEWTON, Christopher, William , RODINI, David, J. , ADKINS, Quinghong, Fu , SIKKEMA, Doetze, Jakob
CPC分类号: C08G75/32 , C08G73/0627 , C08G73/18 , C08G73/22 , D01F6/74
-
-
公开(公告)号:EP1877466A1
公开(公告)日:2008-01-16
申请号:EP06739679.6
申请日:2006-03-27
发明人: ALLEN, Steven, R. , MOORE, Stephen, D. , NEWTON, Christopher, William , RODINI, David, J. , ADKINS, Quinghong, Fu , SIKKEMA, Doetze, Jakob
CPC分类号: C08G75/32 , C08G73/0627 , C08G73/18 , C08G73/22 , D01F6/74
摘要: The present invention concerns a process for making a polyareneazole polymer, comprising the steps of : a) contacting azole-forming monomers, preferably 2, 3, 5, 6-tetraaminopyridine and 2,5-dihydroxyterephthalic acid metal powder, and optionally P2O5, in polyphosphoric acid to form a mixture; b) blending the mixture at a temperature of from 50°C to 110°C; c) further blending the mixture at a temperature of up to 145°C to form a solution comprising an oligomer; d) optionally, degassing the solution; and e) reacting the oligomer solution at a temperature of 160°C to 250°C for a time sufficient to form a polymer.
-
公开(公告)号:EP1863957B1
公开(公告)日:2012-06-13
申请号:EP06748889.0
申请日:2006-03-27
发明人: ALLEN, Steven, R. , MOORE, Stephen, D. , NEWTON, Christopher, W. , RODINI, David, J. , SIKKEMA, Doetze Jakob
CPC分类号: D01D10/06 , D01F6/74 , Y10T428/2913
摘要: The present invention relates to processes for hydrolyzing polyphosphoric acid in a fiber and the removal of hydrolyzed polyphosphoric acid from the fiber.
-
公开(公告)号:EP0934434A1
公开(公告)日:1999-08-11
申请号:EP97913738.0
申请日:1997-10-22
CPC分类号: D01F6/605
摘要: A process is disclosed for making para-aramid filaments of especially high strength by extruding a solution of para-aramid through fine capillaries and drying the resulting filaments under high tension.
-
-
公开(公告)号:EP1866467A2
公开(公告)日:2007-12-19
申请号:EP06799896.3
申请日:2006-03-27
发明人: ALLEN, Steven, R. , MOORE, Stephen, D. , NEWTON, Christopher, William , RODINI, David, J. , SIKKEMA, Doetze Jakob
CPC分类号: D01F6/74
摘要: The present invention concerns a process for making a polyareneazole multifilament yarn comprising: a) extruding a solution comprising polyareneazole polymer and polyphosphoric acid through a plurality of orifices to produce filaments; b) forming a multifilament yarn from said filaments; c) hydrolyzing at least some of the polyphosphoric acid in the yarn by heating the yarn to a temperature above about 120 0C for up to about two minutes; d) washing at least some of the hydrolyzed polyphosphoric acid from the yarn; e) drying the washed yarn; f) optionally, heating the yarn above about 300 0C, and g) collecting the yarn at a speed of at least about 50 meters per minute.
-
-
-
-
-
-
-
-