TEMPERATURE-STABLE CAST-IRON ALLOY AND ITS USE
    1.
    发明公开
    TEMPERATURE-STABLE CAST-IRON ALLOY AND ITS USE 审中-公开
    温哥华(GUSSEISENLEGIERUNG)温哥华(VERWENDUNG DAVON)

    公开(公告)号:EP2059622A1

    公开(公告)日:2009-05-20

    申请号:EP07766720.2

    申请日:2007-06-12

    申请人: FLSmidth A/S

    IPC分类号: C22C37/08

    CPC分类号: C22C37/08 C22C37/10

    摘要: A description is given of a temperature-stable cast-iron alloy having high wear resistance at temperatures between 500 and 900° C. The alloy is characterized in that it has the following composition expressed in weight percentages: chromium: 15.0-20.0 %, carbon: 1.0-2.0 %, manganese: 1.5-2.0 %, silicon: 0.8-1.2 %, nickel: 8.0-10.0 %, molybdenum: 0.8-1.2 % balance iron and unavoidable metallic and non-metallic contaminants where the non-metallic contaminants comprise nitrogen, oxygen, phosphorous and sulphur. Hereby is obtained a cast-iron alloy which has a higher wear resistance and a reduced tendency to form the undesirable sigma phase when heated to temperatures between 500 and 900 °C as compared to the known allows.

    摘要翻译: 给出了在500和900℃之间具有高耐磨性的温度稳定的铸铁合金的描述。该合金的特征在于其具有以重量百分比表示的以下组成:铬:15.0-20.0%,碳 :1.0-2.0%,锰:1.5-2.0%,硅:0.8-1.2%,镍:8.0-10.0%,钼:0.8-1.2%的铁和不可避免的金属和非金属污染物,其中非金属污染物包括 氮,氧,磷和硫。 因此获得了一种铸铁合金,其具有较高的耐磨性,并且与已知的允许相比,当加热至500-900℃之间的温度时,形成不希望的σ相的倾向降低。