公开(公告)号:EP0102085A3
公开(公告)日:1986-02-05
申请号:EP83108541
申请日:1983-08-30
IPC分类号: G21K04/00
CPC分类号: G21K4/00 , C09K11/02 , C09K11/7771
摘要: A radiographic intensifying screen comprising a support and a phosphor-containing resin layer provided thereon, in which the void ratio of said phosphor-containing resin layer is reduced in comparison with an ordinarily prepared phosphor-containing resin layer having the same binder-phosphor ratio and formed by a coating procedure conducted under an atmospheric pressure. The void ratio is not more than 85 % of the void ratio of the ordinarily prepared phosphor-containing resin layer for a phosphor-containing resin layer in which contains a resinous binder and a phosphor in a weight ratio of 1 : 1 to 1 : 25, the ration of 1 : 25 being exclusive, and the void ratio is not more than 90 % for a phosphor-containing resin layer in which contains a resinous binder and a phosphor in a weight ratio of 1 : 25 to 1 : 100.