公开(公告)号:EP3158095A4
公开(公告)日:2017-04-26
申请号:EP08864853
申请日:2008-12-19
申请人: GBC METALS LLC , WIELAND-WERKE AG
发明人: MUTSCHLER RALPH A , ROBINSON PETER WILLIAM , TYLER DEREK E , KAUFLER ANDREA , KUHN HANS ACHIM , HOFMANN UWE
摘要: A copper base alloy having an improved combination of yield strength and electrical conductivity consisting essentially of between about 1.0 and about 6.0 weight percent Ni, up to about 3.0 weight percent Co, between about 0.5 and about 2.0 weight percent Si, between about 0.01 and about 0.5 weight percent Mg, up to about 1.0 weight percent Cr, up to about 1.0 weight percent Sn, and up to about 1.0 weight percent Mn, the balance being copper and impurities, the alloy processed to have a yield strength of at least about 137 ksi, and an electrical conductivity of at least about 25% IACS.
摘要翻译: 一种具有改进的屈服强度和电导率组合的铜基合金,其基本上由约1.0至约6.0重量%的Ni,至多约3.0重量%的Co,约0.5至约2.0重量%的Si,约0.01至约 0.5重量%的Mg,至多约1.0重量%的Cr,至多约1.0重量%的Sn和至多约1.0重量%的Mn,余量为铜和杂质,合金的加工屈服强度为至少约137 ksi,电导率至少约为25%IACS。