Polycarbonate formulation and carrier for semiconductor wafers
    3.
    发明公开
    Polycarbonate formulation and carrier for semiconductor wafers 审中-公开
    聚碳酸酯和Halbleiterplättchenträger

    公开(公告)号:EP0924260A2

    公开(公告)日:1999-06-23

    申请号:EP98309965.6

    申请日:1998-12-04

    IPC分类号: C08L69/00

    摘要: An aromatic polycarbonate composition and articles made from same having less than 300 parts per billion each of ionic impurities, particularly Sulfate and Chloride ions prepared by devolatilizing the ionic impurites from a polycarbonate composition employing an aqueous medium of about 1% by weight based on the weight of the polycarbonate composition. Preferably the devolatilizing is carried out in an extruder during compounding the polycarbonate composition and preferably under a vacuum. Also, the extruded strands of polycarbonate resin are quenched in a water bath having a Sulfate and Chloride ion content of less then 300 ppb each.

    摘要翻译: 芳族聚碳酸酯组合物及其制备的制品具有小于300重量份的离子杂质,特别是硫酸盐和氯离子,其通过使用基于重量的约1重量%的水性介质从聚碳酸酯组合物脱挥发分而制备 的聚碳酸酯组合物。 优选地,在组合聚碳酸酯组合物期间,优选在真空下,在挤出机中进行脱挥发分。 此外,聚碳酸酯树脂的挤出股线在每个硫酸根和氯离子含量小于300ppb的水浴中淬火。

    Reducing ionic impurities content in polycarbonate resins
    7.
    发明公开
    Reducing ionic impurities content in polycarbonate resins 失效
    聚碳酸酯中的Verminderung ionischer Verunreinigungen

    公开(公告)号:EP0870791A2

    公开(公告)日:1998-10-14

    申请号:EP98302394.6

    申请日:1998-03-27

    IPC分类号: C08G64/40

    摘要: An aromatic polycarbonate composition having less than 300 parts per billion each of ionic impurities, particularly sulfate and chloride ions is obtained by devolatilizing the ionic impurities from a polycarbonate composition employing an aqueous medium of about 1% by weight based on the weight of the polycarbonate composition. Preferably the devolatilizing is carried out in an extruder during compounding the polycarbonate composition and preferably under a vacuum. Also, the extruded strands of polycarbonate resin are quenched in a water bath having a sulfate and chloride ion content of less than 300 ppb each.

    摘要翻译: 通过使用基于聚碳酸酯组合物重量的约1重量%的水性介质的聚碳酸酯组合物的离子化分离来获得具有小于300ppm的离子杂质,特别是硫酸根离子和氯离子的芳族聚碳酸酯组合物 。 优选地,在组合聚碳酸酯组合物期间,优选在真空下,在挤出机中进行脱挥发分。 此外,聚碳酸酯树脂的挤出股线在具有小于300ppb的硫酸盐和氯离子含量的水浴中淬火。