公开(公告)号:EP2551944A3
公开(公告)日:2013-02-27
申请号:EP12177521.7
申请日:2012-07-23
发明人: FUNATO, Takayuki , OKADA, Yuichi
CPC分类号: H01M4/364 , H01M4/56 , H01M4/57 , H01M4/583 , H01M10/121
摘要: A lead-acid battery includes a positive electrode plate including a positive electrode grid and a positive active material filled in the positive electrode grid and formed in advance, a negative electrode plate 2 including a negative electrode grid 4 and a negative active material 6 filled in the negative electrode grid 4 and formed in advance, and an electrolyte solution. The positive active material contains a tin compound in an amount of 0.5% by mass to 3.0% by mass (inclusive) on a metal tin basis, and the negative active material 6 contains carbon black in an amount of 0.4% by mass to 2.0% by mass (inclusive). Shrinkage of the negative active material 6 in a thickness direction in a charge-discharge cycle is prevented to improve the charge-discharge life performance.
-
公开(公告)号:EP2551944A2
公开(公告)日:2013-01-30
申请号:EP12177521.7
申请日:2012-07-23
发明人: FUNATO, Takayuki , OKADA, Yuichi
CPC分类号: H01M4/364 , H01M4/56 , H01M4/57 , H01M4/583 , H01M10/121
摘要: A lead-acid battery includes a positive electrode plate including a positive electrode grid and a positive active material filled in the positive electrode grid and formed in advance, a negative electrode plate 2 including a negative electrode grid 4 and a negative active material 6 filled in the negative electrode grid 4 and formed in advance, and an electrolyte solution. The positive active material contains a tin compound in an amount of 0.5% by mass to 3.0% by mass (inclusive) on a metal tin basis, and the negative active material 6 contains carbon black in an amount of 0.4% by mass to 2.0% by mass (inclusive). Shrinkage of the negative active material 6 in a thickness direction in a charge-discharge cycle is prevented to improve the charge-discharge life performance.
摘要翻译: 铅酸电池包括:正极板,其包括正极栅极和填充在正极栅极中并预先形成的正极活性材料;负极板2,其包括负极栅极4和填充在负极栅极4中的负极活性材料6 负电极格栅4并且预先形成,以及电解质溶液。 正极活性物质以金属锡为基准含有0.5质量%以上3.0质量%以下的锡化合物,负极活性物质6含有0.4质量%以上且2.0质量%以下的炭黑, (包括)。 防止充放电循环中的负极活性物质6在厚度方向上的收缩,从而提高充放电寿命性能。
-
公开(公告)号:EP2551944B1
公开(公告)日:2013-10-30
申请号:EP12177521.7
申请日:2012-07-23
发明人: FUNATO, Takayuki , OKADA, Yuichi
CPC分类号: H01M4/364 , H01M4/56 , H01M4/57 , H01M4/583 , H01M10/121
-
-