UV curable non-crystalline acetal terpolymers
    2.
    发明公开
    UV curable non-crystalline acetal terpolymers 失效
    紫外线可固化非晶态乙缩醛

    公开(公告)号:EP0308045A3

    公开(公告)日:1989-06-14

    申请号:EP88306455.2

    申请日:1988-07-14

    CPC分类号: C08G2/00 C08F283/06

    摘要: Ultraviolet curable terpolymers of trioxane, from at least 65 weight percent to about 75 weight percent of 1,3-dioxolane and from about 2 weight percent to about 20 weight percent of a monoethylenically unsaturated aliphatic diol formal having at least 4 carbon atoms in its main chain, e.g., 4,7-dehydro- 1,3-­dioxepin, which are non-crystalline at room temperature or above are disclosed. These terpolymers, when admixed with a multifunctional crosslinking monomer, e.g., a multifunctional acrylate such as 1,6-hexanediol diacrylate, and a photosensitizer, e.g., a benzoin compound such as benzoin isobutyl ether, can be cured to an insoluble, non-tacky, rubbery state using UV radiation. The thus-cured polymeric materials form useful crosslinked films, and when cryogenically ground to a suitable small particle size can be blended with conventionally prepared crystalline oxymethylene homo-, co- and terpolymers to improve the latters' impact properties.

    Low Tg non-crystalline acetal copolymers
    3.
    发明公开
    Low Tg non-crystalline acetal copolymers 失效
    Nichtkristalline乙缩醛共聚物Tg。

    公开(公告)号:EP0308186A2

    公开(公告)日:1989-03-22

    申请号:EP88308465.9

    申请日:1988-09-14

    IPC分类号: C08G2/24 C08G2/18 C08L59/00

    CPC分类号: C08G2/00

    摘要: Low Tg copolymers of trioxane and 1,3-dioxolane which have a dioxolane content greater than 65 mol percent and less than about 75 mol percent and an IV of from about 1.0 to about 2.3, and which are non-crystalline at room temperature or above, are disclosed. These polymers, when blended with crystalline oxymethylene polymers, improve the latter's impact properties. They can also be used as adhesives for crystalline oxymethylene polymers.

    摘要翻译: 三恶烷和1,3-二氧戊环的低Tg共聚物的二氧戊环含量大于65mol%且小于约75mol%,IV为约1.0至约2.3,并且在室温或更高温度下为非结晶 ,被披露。 当与结晶甲醛聚合物共混时,这些聚合物改善了后者的冲击性能。 它们也可以用作结晶甲醛聚合物的粘合剂。

    Low Tg non-crystalline acetal copolymers
    5.
    发明公开
    Low Tg non-crystalline acetal copolymers 失效
    低TG非晶体乙烯共聚物

    公开(公告)号:EP0308186A3

    公开(公告)日:1989-06-14

    申请号:EP88308465.9

    申请日:1988-09-14

    IPC分类号: C08G2/24 C08G2/18 C08L59/00

    CPC分类号: C08G2/00

    摘要: Low Tg copolymers of trioxane and 1,3-dioxolane which have a dioxolane content greater than 65 mol percent and less than about 75 mol percent and an IV of from about 1.0 to about 2.3, and which are non-crystalline at room temperature or above, are disclosed. These polymers, when blended with crystalline oxymethylene polymers, improve the latter's impact properties. They can also be used as adhesives for crystalline oxymethylene polymers.

    UV curable non-crystalline acetal terpolymers
    6.
    发明公开
    UV curable non-crystalline acetal terpolymers 失效
    UV-härtbarenichtkristalline Acetalterpolymere。

    公开(公告)号:EP0308045A2

    公开(公告)日:1989-03-22

    申请号:EP88306455.2

    申请日:1988-07-14

    CPC分类号: C08G2/00 C08F283/06

    摘要: Ultraviolet curable terpolymers of trioxane, from at least 65 weight percent to about 75 weight percent of 1,3-dioxolane and from about 2 weight percent to about 20 weight percent of a monoethylenically unsaturated aliphatic diol formal having at least 4 carbon atoms in its main chain, e.g., 4,7-dehydro- 1,3-­dioxepin, which are non-crystalline at room temperature or above are disclosed. These terpolymers, when admixed with a multifunctional crosslinking monomer, e.g., a multifunctional acrylate such as 1,6-hexanediol diacrylate, and a photosensitizer, e.g., a benzoin compound such as benzoin isobutyl ether, can be cured to an insoluble, non-tacky, rubbery state using UV radiation. The thus-cured polymeric materials form useful crosslinked films, and when cryogenically ground to a suitable small particle size can be blended with conventionally prepared crystalline oxymethylene homo-, co- and terpolymers to improve the latters' impact properties.

    摘要翻译: 三恶烷的紫外线固化三元共聚物,其至少65重量%至约75重量%的1,3-二氧戊环和约2重量%至约20重量%的其主要具有至少4个碳原子的单烯键式不饱和脂族二醇缩甲醛 链,例如4,7-脱氢-1,3-二氧杂环庚烯,其在室温或以上是非结晶的。 当与多官能交联单体(例如多官能丙烯酸酯如1,6-己二醇二丙烯酸酯)和光敏剂(例如苯偶姻化合物如苯偶姻异丁基醚)混合时,这些三元共聚物可以固化成不溶性,非粘性 ,使用紫外线辐射的橡胶状态。 如此固化的聚合物材料形成有用的交联膜,并且当低温研磨成合适的小粒径时,可与常规制备的结晶甲醛均聚物,共聚物和三元共聚物共混以改善后者的冲击性能。

    Articles utilizing acetal copolymer bonding resins
    7.
    发明公开
    Articles utilizing acetal copolymer bonding resins 失效
    使用乙烯共聚物粘结树脂的文章

    公开(公告)号:EP0364207A3

    公开(公告)日:1991-10-02

    申请号:EP89310339.0

    申请日:1989-10-10

    IPC分类号: C09J159/00

    摘要: There are provided new articles comprising elements having surfaces bonded together with a bonding resin which is an elastomeric copolymer of about 15 to 45 mol %, preferably about 25 to 35 mol % trioxane, about 55 to 85 mol %, preferably about 65 to 75 mol % of 1,3-dioxolane, said mol percents based on the total of trioxane and 1,3-dioxolane, and about 0.005 to 0.15 wt.%, preferably about 0.05 to 0.12 wt.% of 1,4-butanediol diglycidyl ether of butadiene diepoxide as a bifunctional monomer, based on the total weight of copolymer. Preferably, at least one of said surfaces, and more preferably at least two of said surfaces bonded to each other are of a crystalline acetal polymer comprising at least 85 mol % of polymerized oxymethylene unit.

    摘要翻译: 提供了新的物品,其包括具有与粘合树脂结合在一起的元件,所述粘合树脂是约15至45摩尔%,优选约25至35摩尔%三恶烷,约55至85摩尔%,优选约65至75摩尔的弹性体共聚物 %的1,3-二氧戊环,基于三恶烷和1,3-二氧戊环的总量的摩尔百分比,以及约0.005至0.15重量%,优选约0.05至0.12重量%的1,4-丁二醇二缩水甘油醚 丁二烯二环氧化物作为双官能单体,基于共聚物的总重量。 优选地,所述表面中的至少一个,更优选至少两个彼此键合的表面是包含至少85摩尔%聚合的甲醛单元的结晶性缩醛聚合物。

    Acetal polymer compositions of high impact strength
    8.
    发明公开
    Acetal polymer compositions of high impact strength 失效
    Polyacetalzusammensetzungen mit hoher Schlagfestigkeit。

    公开(公告)号:EP0409464A2

    公开(公告)日:1991-01-23

    申请号:EP90307498.7

    申请日:1990-07-09

    IPC分类号: C08L59/04

    摘要: A composition is provided comprising a major amount of normally crystalline acetal polymer and lower amounts than said crystalline acetal polymer of a thermoplastic polyurethane and a normally non-crystalline acetal copolymer of monomers comprising about 15 to 45 mol % of trioxane and about 55 to 85 mol % of 1,3-dioxolane based on the total of trioxane and 1,3-dioxolane. The composition may be molded into articles having high impact strength.

    摘要翻译: 提供了一种组合物,其包含主要量的通常结晶的缩醛聚合物,并且比所述热塑性聚氨酯的结晶缩醛聚合物和通常非结晶的包含约15至45mol%三恶烷和约55至85mol 基于三恶烷和1,3-二氧戊环的总量的1,3-二氧戊环的%。 组合物可以模制成具有高冲击强度的制品。

    Articles utilizing acetal copolymer bonding resins
    9.
    发明公开
    Articles utilizing acetal copolymer bonding resins 失效
    Gegenstände,die ein Bindeharz aus Acetalcopolymer enthalten。

    公开(公告)号:EP0364207A2

    公开(公告)日:1990-04-18

    申请号:EP89310339.0

    申请日:1989-10-10

    IPC分类号: C09J159/00

    摘要: There are provided new articles comprising elements having surfaces bonded together with a bonding resin which is an elastomeric copolymer of about 15 to 45 mol %, preferably about 25 to 35 mol % trioxane, about 55 to 85 mol %, preferably about 65 to 75 mol % of 1,3-dioxolane, said mol percents based on the total of trioxane and 1,3-dioxolane, and about 0.005 to 0.15 wt.%, preferably about 0.05 to 0.12 wt.% of 1,4-butanediol diglycidyl ether of butadiene diepoxide as a bifunctional monomer, based on the total weight of copolymer. Preferably, at least one of said surfaces, and more preferably at least two of said surfaces bonded to each other are of a crystalline acetal polymer comprising at least 85 mol % of polymerized oxymethylene unit.

    摘要翻译: 提供了新的物品,其包括具有与粘合树脂结合在一起的元件,所述粘合树脂是约15至45摩尔%,优选约25至35摩尔%三恶烷,约55至85摩尔%,优选约65至75摩尔的弹性体共聚物 %的1,3-二氧戊环,基于三恶烷和1,3-二氧戊环的总量的摩尔百分比,以及约0.005至0.15重量%,优选约0.05至0.12重量%的1,4-丁二醇二缩水甘油醚 丁二烯二环氧化物作为双官能单体,基于共聚物的总重量。 优选地,所述表面中的至少一个,更优选至少两个彼此键合的表面是包含至少85摩尔%聚合的甲醛单元的结晶性缩醛聚合物。