    摘要: A consecutive molding method for crystallized glass comprises: a melting process to obtain molten glass by melting glass raw materials; a molding process to obtain a band-shaped plate glass by roll forming the molten glass to become band-shaped; a crystallization process to obtain a band-shaped crystallized glass plate by conducting thermal treatment on the band-shaped plate glass to crystallize it; and a cutting process to cut the band-shaped crystallized glass plate, wherein the crystallization process includes: a crystal nucleus-formation process to form crystal nuclei in the band-shaped plate glass obtained in the molding process by disposing the band-shaped plate glass in the atmosphere of a crystal nucleus-formation temperature and retaining it at the temperature; a temperature-raising process to raise the temperature of the band-shaped plate glass where crystal nuclei have been formed to a crystal-growth temperature; a crystal-growth process to retain the band-shaped plate glass where crystal nuclei have been formed at the crystal-growth temperature such that the glass is crystallized to produce a band-shaped crystallized glass plate; and a slow-cooling process to slowly cool down the band-shaped crystallized glass plate.

    摘要翻译: 一种用于结晶玻璃的连续模制方法包括:通过熔化玻璃原料来获得熔融玻璃的熔融过程; 通过将所述熔融玻璃辊成形为带状来获得带状平板玻璃的成型工艺; 通过对所述带状平板玻璃进行热处理使其结晶而获得带状结晶玻璃板的结晶工艺; 以及切断工序,切断所述带状结晶化玻璃板,所述结晶化工序包括:在所述成型工序中得到的带状平板玻璃中,通过配置所述带状平板玻璃而形成晶核的晶核形成工序 在晶核形成温度的气氛中并保持在该温度下; 将形成晶核的带状平板玻璃的温度升高至晶体生长温度的升温过程; 在结晶生长温度下保持形成晶核的带状平板玻璃的晶体生长工艺,使得玻璃结晶以产生带状结晶玻璃板; 以及缓慢冷却带状结晶玻璃板的过程。

    Method for making crystallized glass by rolling and heat treating and apparatus
    3.
    发明公开
    Method for making crystallized glass by rolling and heat treating and apparatus 审中-公开
    过程用于通过轧制和热处理,以及装置制备结晶化玻璃

    公开(公告)号:EP2524902A2

    公开(公告)日:2012-11-21

    申请号:EP12001851.0

    申请日:2012-03-19

    IPC分类号: C03B13/04 C03B25/08 C03B32/02

    摘要: A consecutive molding method for crystallized glass comprises: a melting process to obtain molten glass by melting glass raw materials; a molding process to obtain a band-shaped plate glass by roll forming the molten glass to become band-shaped; a crystallization process to obtain a band-shaped crystallized glass plate by conducting thermal treatment on the band-shaped plate glass to crystallize it; and a cutting process to cut the band-shaped crystallized glass plate, wherein the crystallization process includes: a temperature-raising process to produce the band-shaped crystallized glass plate by disposing the band-shaped plate glass obtained in the molding process, in the atmosphere of a crystal nucleus-formation temperature and raising the temperature to a crystal-growth temperature or above to grow crystals as well as form crystal nuclei; and a slow-cooling process to slowly cool down the band-shaped crystallized glass plate.

    摘要翻译: 对结晶化玻璃的一个连续成型方法,包括:熔融过程通过熔化玻璃原料,得到熔融玻璃; 模制工艺,以获得由辊轧成形的熔融玻璃,成为带状的带状平板玻璃; 结晶过程通过进行对带状平板玻璃使其结晶热处理以获得带状结晶化玻璃板; 和切割工艺切割带状结晶化玻璃板,worin结晶过程包括:升温步骤通过设置在模制过程获得的带状平板玻璃生产带状结晶化玻璃板,在 晶核形成温度的气氛中,升温到结晶成长温度或以上,以生长晶体以及形式晶核; 和慢冷却过程缓慢地冷却带状结晶化玻璃板。

    Method for making crystallized glass by rolling and heat treating and apparatus
    4.
    发明公开
    Method for making crystallized glass by rolling and heat treating and apparatus 审中-公开
    过程用于通过轧制和热处理,以及装置制备结晶化玻璃

    公开(公告)号:EP2524901A2

    公开(公告)日:2012-11-21

    申请号:EP12001849.4

    申请日:2012-03-19

    IPC分类号: C03B13/04 C03B25/08 C03B32/02

    摘要: A consecutive molding method for crystallized glass comprises: a melting process to obtain molten glass by melting glass raw materials; a molding process to obtain a band-shaped plate glass by roll forming the molten glass to become band-shaped; a crystallization process to obtain a band-shaped crystallized glass plate by conducting thermal treatment on the band-shaped plate glass to crystallize it; and a cutting process to cut the band-shaped crystallized glass plate, wherein the crystallization process includes: a crystal nucleus-formation process to form crystal nuclei in the band-shaped plate glass obtained in the molding process by disposing the band-shaped plate glass in the atmosphere of a crystal nucleus-formation temperature and retaining it at the temperature; a temperature-raising process to raise the temperature of the band-shaped plate glass where crystal nuclei have been formed to a crystal-growth temperature; a crystal-growth process to retain the band-shaped plate glass where crystal nuclei have been formed at the crystal-growth temperature such that the glass is crystallized to produce a band-shaped crystallized glass plate; and a slow-cooling process to slowly cool down the band-shaped crystallized glass plate.

    摘要翻译: 对结晶化玻璃的一个连续成型方法,包括:熔融过程通过熔化玻璃原料,得到熔融玻璃; 模制工艺,以获得由辊轧成形的熔融玻璃,成为带状的带状平板玻璃; 结晶过程通过进行对带状平板玻璃使其结晶热处理以获得带状结晶化玻璃板; 和切割工艺切割带状结晶化玻璃板,worin结晶过程包括:晶核形成过程,以形成在通过设置带状平板玻璃在成型工序中得到的带状板玻璃的晶核 在晶核形成温度的气氛,并且在该温度下保持它; 的升温过程,以提高带状平板玻璃,其中晶核已形成于晶体生长温度的温度; 晶体生长过程中保留了带状平板玻璃,其中晶核已经在检查做的玻璃结晶化,以产生带状结晶化玻璃板的晶体生长温度形成; 和慢冷却过程缓慢地冷却带状结晶化玻璃板。