摘要:
This invention provides polypropylene resin compositions exhibiting a strongly improved balance of physical properties in comparison to related polypropylene materials. The materials can be used in both interior and exterior parts of automobiles, have excellent thin-wall moldability and can effectively reduce generation of flow marks. Particularly, it provides a polypropylene resin composition which comprises specified amounts of (A) a specific ethylene-propylene block copolymer, (B) a specific thermoplastic elastomer and (C) talc, wherein it has specified values of physical properties measured by ASTM and has a degree of b-axis orientation of 720 or more which is calculated from the ratio of differential peak intensities measured by wide-angle X-ray diffraction of the central area of an ASTM No. 1 dumbbell prepared by injection molding.
摘要:
There is provided a thermoplastic resin composition comprising the following components (A) to (E):
component (A) : 50 to 74.7% by weight of a propyleneethylene block copolymer resin containing a propylene homopolymer moiety having a melt flow rate of 20 to 200 g/10 min. and an isotactic pentad fraction of at least 0.98, the block copolymer having a melt flow rate of 10 to 100 g/10 min. and a ratio of the weight average molecular weight to the number average molecular weight of 5 to 7, component (B): 5 to 10% by weight of an ethylene-octene random copolymer having a melting temperature of 40 to 60°C and a melt flow rate of 0.5 to 15 g/10 min., component (C): 5 to 10% by weight of an ethylene-butene random copolymer not having a melting temperature of 35°C or above and having a melt flow rate of 0.5 to 15 g/10 min., component (D): 0.3 to 5% by weight of an elastomer, the elastomer being either one comprising a block structure represented by the following formula [I] and/or the following formula [II] and having a melting temperature of 80 to 110°C, a melt flow rate of 0.5 to 20 g/10 min., a polyethylene crystal moiety content of 20 to 40% by weight, and a random elastomer moiety content of 60 to 80% by weight, or one comprising a block structure represented by the following formula [III], the following formula [IV] and/or the following formula [V] and having a melt flow rate of not more than 15 g/10 min. and a polystyrene moiety content of 10 to 40% by weight and a random elastomer moiety content of 60 to 90% by weight:
polyethylene-(ethylene/butene random elastomer)-polyethylene [I]
polyethylene-(ethylene/butene random elastomer) [II]
polystyrene-(ethylene/butene random elastomer)-polystyrene [III]
polystyrene-(ethylene/propylene random elastomer)-polystyrene [IV]
polystyrene-(ethylene/propylene random elastomer) [V];
and component (E): 15 to 25% by weight of a talc having an average particle diameter of up to 5 µm and a specific surface area of at least 3.5 m 2 /g.
摘要:
A resin composition having excellent paint coatability comprising: (A) 50-80 weight % of a multi-stage polymerized propylene-ethylene block copolymer consisting essentially of (i) a propylene homopolymer portion, (ii) a propylene-ethylene random copolymer portion, and (iii) an ethylene homopolymer portion, said propylene-ethylene block copolymer being characterized that an intrinsic viscosity of said propylene homopolymer portion (i) is 0.9-1.2 dl/g, an intrinsic viscosity of said propylene-ethylene random copolymer portion (ii) is 4.0 dl/g or more, and an ethylene content of said propylene-ethylene random copolymer portion (ii) is 30-70 weight %; (B) 20-40 weight % of an ethylene-α-olefin copolymer elastomer; and (C) up to 20 weight % of an inorganic filler.
摘要:
A resin composition having excellent paint coatability comprising:
(A) 50-80 weight % of a multi-stage polymerized propylene-ethylene block copolymer consisting essentially of (i) a propylene homopolymer portion, (ii) a propylene-ethylene random copolymer portion, and (iii) an ethylene homopolymer portion, said propylene-ethylene block copolymer being characterized by the requirement that:
(a) said propylene-ethylene random copolymer portion (ii) has a number-average molecular weight of 20 X 40 4 or more and a weight-average molecular weight of 60 X 10 4 or more; (b) a content of ethylene is 60 weight % or more and a content of said ethylene homopolymer portion (iii) is 40 weight % or more, both based on the total amount (100 weight %) of said propylene-ethylene random copolymer portion (ii) and said ethylene homopolymer portion (iii); or (c) an intrinsic viscosity of said propylene homopolymer portion (i) is 0.9-1.2 dl/g, an intrinsic viscosity of said propylene-ethylene random copolymer portion (ii) is 4.0 dl/g or more, and an ethylene content of said propylene-ethylene random copolymer portion (ii) is 30-70 weight %;
(B) 20-40 weight % of an ethylene-α-olefin copolymer elastomer; and (C) up to 20 weight % of an inorganic filler.
摘要:
A resin composition having excellent paint coatability containing (a) 50-80 weight % of a multi-stage polymerized propylene-ethylene block copolymer consisting essentially of (i) a propylene homopolymer portion, (ii) a propylene-ethylene random copolymer portion, and (iii) an ethylene homopolymer portion, (b) 20-40 weight % of an ethylene- alpha -olefin copolymer elastomer, and (c) 20 weight % or less of an inorganic filler, components in the components (a) and (b), which are soluble in p-xylene at a room temperature, having a number-average molecular weight of 4 x 10 or more and a weight-average molecular weight of 20 x 10 or more.
摘要:
A resin composition having excellent paint coatability containing (a) 50-80 weight % of a multi-stage polymerized propylene-ethylene block copolymer consisting essentially of (i) a propylene homopolymer portion, (ii) a propylene-ethylene random copolymer portion, and (iii) an ethylene homopolymer portion, (b) 20-40 weight % of an ethylene- alpha -olefin copolymer elastomer, and (c) 20 weight % or less of an inorganic filler, components in the components (a) and (b), which are soluble in p-xylene at a room temperature, having a number-average molecular weight of 4 x 10 or more and a weight-average molecular weight of 20 x 10 or more.
摘要:
A resin composition having excellent paint coatability comprising:
(A) 50-80 weight % of a multi-stage polymerized propylene-ethylene block copolymer consisting essentially of (i) a propylene homopolymer portion, (ii) a propylene-ethylene random copolymer portion, and (iii) an ethylene homopolymer portion, said propylene-ethylene block copolymer being characterized that an intrinsic viscosity of said propylene homopolymer portion (i) is 0.9-1.2 dl/g, an intrinsic viscosity of said propylene-ethylene random copolymer portion (ii) is 4.0 dl/g or more, and an ethylene content of said propylene-ethylene random copolymer portion (ii) is 30-70 weight %; (B) 20-40 weight % of an ethylene-α-olefin copolymer elastomer; and (C) up to 20 weight % of an inorganic filler.
摘要:
A resin composition having excellent paint coatability containing (a) 50-80 weight % of a multi-stage polymerized propylene-ethylene block copolymer consisting essentially of (i) a propylene homopolymer portion, (ii) a propylene-ethylene random copolymer portion, and (iii) an ethylene homopolymer portion, (b) 20-40 weight % of an ethylene-α-olefin copolymer elastomer, and (c) 20 weight % or less of an inorganic filler, components in the components (a) and (b), which are soluble in p-xylene at a room temperature, having a number-average molecular weight of 4 x 10⁴ or more and a weight-average molecular weight of 20 x 10⁴ or more.