Process for producing heat-resistant intermetallic compound Ni3Al foil and product foil obtained
    1.
    发明公开
    Process for producing heat-resistant intermetallic compound Ni3Al foil and product foil obtained 审中-公开
    一种用于根据该制造方法制造的片状的耐热金属间化合物Ni3Al金属和产品的方法,

    公开(公告)号:EP1094135A1

    公开(公告)日:2001-04-25

    申请号:EP00309293.9

    申请日:2000-10-20

    摘要: A process for producing a heat-resistant intermetallic compound Ni 3 Al foil having a room-temperature ductility, which comprises a first step of arc-melting an alloy having a chemical composition containing Ni as a main component and Al to form a starting rod, a second step of growing the starting rod in columnar crystal form by unidirectional solidification, a third step of cutting out the unidirectionally solidified rod to form a plate, and a fourth step of cold-rolling the plate cut at room temperature to form a foil. The invention can provide a process for producing a thin Ni 3 Al foil which has a thickness of 200 microns or less and which is excellent in high-temperature strength, oxidation and corrosion resistances and room-temperature ductility.

    摘要翻译: 一种用于制造耐热金属间化合物Ni3Al金属箔具有室温延展性,其包括具有如下化学成分含有Ni作为主成分和Al,以形成起始棒合金的电弧熔化的第一步骤,第二过程 通过单向凝固,切割出单向凝固棒,以形成板的第三步骤,和的冷轧在室温下将板切割以形成箔的第四步骤中生长柱状晶体形式的起始棒的步骤。 本发明可用于生产薄Ni3Al金属箔的厚度为200微米或更小,提供一种方法和所有其具有优异的高温强度,氧化和腐蚀termoresistencias和室温延展性。