POLYESTER COMPOSITE FIBER WITH EXCELLENT HEAT-SHIELDING PROPERTY AND COLORATION

    公开(公告)号:EP2808428B1

    公开(公告)日:2018-06-13

    申请号:EP13741605.3

    申请日:2013-01-17

    申请人: Kuraray Co., Ltd.

    IPC分类号: D01F8/14 D01F1/10

    摘要: To provide a polyester composite fiber having a heat-shielding property due to high reflectance in an infrared wavelength range (800 to 3000 nm) easy to be changed into thermal energy, and having color development property comparable to that of conventional polyester fibers. The composite fiber is a core-sheath type composite fiber including a core component and a sheath component of 10: 90 to 30: 70 (mass ratio). The core component includes a thermoplastic polymer including a sunlight shielding material having an average particle size of 0.5 µm or smaller in 8-70 wt%. The sheath component includes a polyester-type polymer including heat-shielding fine particles in 0.5-10 wt%, the heat-shielding fine particles capable of maintaining color development property and having an average particle size of 0.1 µm or smaller which is smaller than that of the sunlight shielding material.

    COMPOSITE FIBER
    3.
    发明公开
    COMPOSITE FIBER 审中-公开

    公开(公告)号:EP3901335A1

    公开(公告)日:2021-10-27

    申请号:EP19900004.3

    申请日:2019-12-04

    申请人: Kuraray Co., Ltd.

    IPC分类号: D01F8/04

    摘要: The present invention relates to a composite fiber for obtaining a fiber having a strength at 100% elongation of 0.04 cN/dtex or less,
    wherein the composite fiber is composed of component X comprising a polyvinyl-based thermoplastic elastomer, or a thermoplastic polyurethane elastomer having a glass transition temperature of 0°C or lower, and component Y which is an easily soluble thermoplastic polymer,
    wherein the composite ratio (mass ratio) X:Y of the component X and the component Y is within the range of from 90:10 to 50:50, and
    wherein the composite fiber has a core-sheath structure in which the component X constitutes the core component, and the component Y constitutes the sheath component, in a cross section of the fiber.

    POLYAMIDE FIBERS, METHOD FOR PRODUCING SAME AND FIBER STRUCTURE

    公开(公告)号:EP4060100A1

    公开(公告)日:2022-09-21

    申请号:EP20886825.7

    申请日:2020-11-11

    申请人: Kuraray Co., Ltd.

    IPC分类号: D01F6/90 C08L77/00

    摘要: Provided is a polyamide fiber having excellent color developability, as well as a method for producing such a polyamide fiber, and a fiber structure. The polyamide fiber comprises a polyamide resin composition comprising a polyamide resin and an amino group-containing color enhancer, the polyamide fiber having terminal amino groups at a concentration of from 5.0 µeq/g to 40.0 µeq/g. Such a fiber can be produced by a production method at least comprising: melt-kneading a polyamide resin composition including a polyamide resin and an amino group-containing color enhancer to give a melt-kneaded product having a predetermined melt viscosity; and spinning the melt-kneaded product to give fibers.

    POLYESTER COMPOSITE FIBER WITH EXCELLENT HEAT-SHIELDING PROPERTY AND COLORATION
    7.
    发明公开
    POLYESTER COMPOSITE FIBER WITH EXCELLENT HEAT-SHIELDING PROPERTY AND COLORATION 有权
    多功能食品消化系统麻省理工学院麻省理工学院

    公开(公告)号:EP2808428A1

    公开(公告)日:2014-12-03

    申请号:EP13741605.3

    申请日:2013-01-17

    申请人: Kuraray Co., Ltd.

    IPC分类号: D01F8/14

    摘要: To provide a polyester composite fiber having a heat-shielding property due to high reflectance in an infrared wavelength range (800 to 3000 nm) easy to be changed into thermal energy, and having color development property comparable to that of conventional polyester fibers. The composite fiber is a core-sheath type composite fiber including a core component and a sheath component of 10: 90 to 30: 70 (mass ratio). The core component includes a thermoplastic polymer including a sunlight shielding material having an average particle size of 0.5 µm or smaller in 8-70 wt%. The sheath component includes a polyester-type polymer including heat-shielding fine particles in 0.5-10 wt%, the heat-shielding fine particles capable of maintaining color development property and having an average particle size of 0.1 µm or smaller which is smaller than that of the sunlight shielding material.

    摘要翻译: 为了提供由于红外波长范围(800〜3000nm)的高反射率而具有热屏蔽性的聚酯复合纤维,易于变成热能,并且具有与常规聚酯纤维相当的显色性能。 复合纤维是包含核成分和护皮成分为10:90〜30:70(质量比)的芯鞘型复合纤维。 核心部件包括热塑性聚合物,其包含8-70重量%的平均粒径为0.5μm以下的阳光遮蔽材料。 护套成分包括含有0.5〜10重量%的遮光性微粒的聚酯型聚合物,能够保持显色性且平均粒径为0.1μm以下的遮光性微粒小于 的阳光屏蔽材料。