METHOD FOR PREPARING SUPPORTED METALLOCENE CATALYST
    4.
    发明公开
    METHOD FOR PREPARING SUPPORTED METALLOCENE CATALYST 审中-公开
    VERFAHREN ZUR HERSTELLUNG EINESGETRÄGERTENMETALLOCENKATALYSATORS

    公开(公告)号:EP3050904A1

    公开(公告)日:2016-08-03

    申请号:EP14865686.1

    申请日:2014-11-28

    申请人: LG Chem, Ltd.

    IPC分类号: C08F4/02 C08F4/6592 C08F10/00

    摘要: The present invention relates to a preparation method of a highly active supported metallocene catalyst which can prepare a polyolefin of high bulk density. More specifically, the present invention provides a method of preparing the supported metallocene catalyst in which one or more metallocene catalysts are loaded on the silica carrier of which the inside is penetrated by more cocatalyst than the prior art and the outside is attached with a substantial amount of the cocatalyst. The catalyst according to the present invention can prepare a polyolefin polymer with improved bulk density and efficiency while maintaining its highly active catalytic characteristic.

    摘要翻译: 本发明涉及一种高活性负载金属茂催化剂的制备方法,该方法可以制备高堆积密度的聚烯烃。 更具体地说,本发明提供一种制备负载型茂金属催化剂的方法,其中一种或多种茂金属催化剂装载在二氧化硅载体上,其内部被比现有技术更多的助催化剂渗透,外部附着有大量的 的助催化剂。 根据本发明的催化剂可以制备具有改进的堆积密度和效率的聚烯烃聚合物,同时保持其高活性催化特性。

    METHOD FOR PREPARING SUPPORTED HYBRID METALLOCENE CATALYST

    公开(公告)号:EP3714975A1

    公开(公告)日:2020-09-30

    申请号:EP19751865.7

    申请日:2019-02-07

    申请人: LG CHEM, LTD.

    摘要: The present disclosure relates to a method for preparing a supported hybrid metallocene catalyst, and the catalyst is prepared by supporting a first metallocene compound, supporting a cocatalyst by a separate-input method in which primarily adding a part at 100 °C to 150 °C and secondarily adding the rest at -5 °C to 40 °C, and then supporting a second metallocene compound, thereby improving a supporting rate of the cocatalyst in the supported catalyst and maintaining high catalytic activity. Therefore, the present disclosure can effectively prepare a polyolefin with improved processability which exhibits increased molecular weight distribution while having high morphology (reduced fine powder), high bulk density and improved settling efficiency.