1.
公开(公告)号:EP4230336A1
公开(公告)日:2023-08-23
申请号:EP21890809.3
申请日:2021-09-17
申请人: Ling Dong Nuclear Power Co., Ltd , China Nuclear Power Technology Research Institute Co., Ltd. , China General Nuclear Power Corporation , CGN Power Co., Ltd.
发明人: XUE, Jiaxiang , LIAO, Yehong , REN, Qisen , LIU, Tong , ZHAI, Jianhan , MA, Haibin , ZHANG, Xiansheng , ZHANG, Yongdong , LI, Rui , LIU, Yang
摘要: A brazing connection method for a silicon carbide cladding, comprising the following steps: S1, using Al and Si as connection materials, providing the connection materials between a cladding pipe and an end plug which are matched with each other, forming a middle connection material of an Al/Si/Al three-layer structure, and forming, by means of the middle connection material, the cladding pipe, and the end plug, an assembly to be connected; and S2, placing said assembly in a vacuum or inert atmosphere for brazing connection, the middle connection material forming a connection layer, and connecting the cladding pipe and the end plug into a whole. The present invention further relates to a silicon carbide cladding formed by the method, a fuel rod comprising same, and a fuel assembly. In the present brazing connection method, Al and Si are used as the connection materials, and the connection layer of the Al/Si/Al three-layer structure is formed between the cladding pipe and the end plug, such that high-strength and reliable connection of the SiC cladding is achieved, and the SiC cladding is good in high-temperature resistance and hydrothermal corrosion resistance, thereby meeting nuclear application requirements.
-
2.
公开(公告)号:EP4230598A1
公开(公告)日:2023-08-23
申请号:EP21890810.1
申请日:2021-09-17
申请人: China Nuclear Power Technology Research Institute Co., Ltd. , Ling Dong Nuclear Power Co., Ltd , China General Nuclear Power Corporation , CGN Power Co., Ltd.
发明人: XUE, Jiaxiang , LIAO, Yehong , REN, Qisen , LIU, Tong , ZHAI, Jianhan , MA, Haibin , ZHANG, Xiansheng , ZHANG, Yongdong , LI, Rui , LIU, Yang
摘要: Disclosed are a solder for connection and a preparation method therefor and a method for connecting a silicon carbide cladding. The solder for connection comprises the following raw materials: a precursor, a glass powder and an organic solvent, wherein the mass ratio of the precursor to the glass powder is 90-98: 2-10. The solder for connection of the present invention is used for connecting a silicon carbide cladding. A glass additive phase formed by the glass powder has good wettability to silicon carbide and a high connection strength. The proportion of the glass powder is adjustable, so that the coefficient of thermal expansion of the glass additive phase is adjustable, and the stress of a joint after connection is controllable. A thick compact connection layer can be realized, facilitating engineering assembly and realizing better air tightness.
-