    摘要: A glass rod (2) for a core or for the core and a cladding is inserted into a glass pipe (1) for the cladding and heated by a heater (3) while the pressure inside the glass pipe (1) is reduced. After at least one of either the glass pipe (1) or the glass rod (2) is elongated, the glass pipe (1) and the glass rod (2) are formed into a single unit, and then the glass pipe (1) and the glass rod (2) are elongated until the outer diameter of the glass pipe (1) becomes a predetermined diameter.

    摘要翻译: 在玻璃管(1)内部的压力减小的同时,用于芯部或芯部和包层的玻璃棒(2)被插入到用于包层的玻璃管(1)中并且由加热器(3)加热。 在玻璃管(1)或玻璃棒(2)中的至少一个拉长后,玻璃管(1)和玻璃棒(2)形成一个单元,然后玻璃管(1) 和玻璃棒(2)伸长,直到玻璃管(1)的外径达到预定的直径。