STEEL PLATE EXHIBITING EXCELLENT WORKABILITY AND METHOD FOR PRODUCING THE SAME
    4.
    发明公开
    STEEL PLATE EXHIBITING EXCELLENT WORKABILITY AND METHOD FOR PRODUCING THE SAME 有权
    凭借出色的切削加工性和方法钢板用于生产

    公开(公告)号:EP1431407A4

    公开(公告)日:2006-01-04

    申请号:EP02736196

    申请日:2002-06-27

    申请人: NIPPON STEEL CORP

    摘要: A steel plate exhibiting excellent workability being used in the panels, suspension system, member, or the like, of an automobile. The steel plate excellent in workability contains C:0.08-0.25%, Si:0.001-1.5%, Mn:0.01-2.0%, P:0.001-0.06%, S:0.05% or less, N:0.001-0.007%, Al:0.008-0.2%, by mass and the remainder of iron and inevitable impurities, characterized in that the average r-value is 1.2 or above, r-value (rL) in the rolling direction is 1.3 or above, r-value (rD) in the direction of 45° with respect to the rolling direction is 0.9 or above, and r-value (rC) in the direction perpendicular to the rolling direction is 1.2 or above. A steel plate and a steel pipe excellent in workability in claim 1, characterized by having the X-ray reflective face random strength ratio of the plate faces {111}, {100}, and {110} at one half thickness of the steel plate set to 2.0 or above, 1.0 or less, and 0.2 or above, respectively, and the methods for producing them.

    摘要翻译: 本发明提供的加工性的钢板优良,所有这些都被用于面板,底盘部件,结构部件等的汽车的,和用于产生所述钢板的方法。 更具体地,本发明是:在钢板加工性优异,在所述钢板为特征的含有:以质量,0:08〜0.25%C,0.001至1.5%的Si,0点01分至2.0%的Mn,0.001〜0.06%,P, 0.05%或更少的S,0.001〜0.007%N和0.008〜0.2%的Al,余量由Fe和不可避免的杂质,并且所述钢板具有1.2或更多的,在r值的平均值r值 轧制方向为1.3以上,在45度与轧制方向的0.9或更大,并且以直角与轧制方向的方向上的r值(R D)的方向上的r值(RH)(RC )为1.2以上; 此外钢板的可加工性优异NACH请求权1,其特征在于在厚度做在ä111ü,ä100ü和ä110ü的方位分量的X射线衍射强度的比为随机的X射线衍射强度的强度上的反射面 所述钢片材的中心分别为2.0以上,1.0以下,0.2以上,; 由所述钢片材的钢管; 和方法用于产生所述钢板和钢管。