Steel material for high strength constant velocity joint intermediate shaft and high strength constant velocity joint intermediate shaft

    公开(公告)号:EP1647608A1

    公开(公告)日:2006-04-19

    申请号:EP05019591.6

    申请日:2005-09-08

    IPC分类号: C22C38/12 C21D9/30

    摘要: A steel material for a high strength constant velocity joint intermediate shaft containing C: 0.46 to 0.52%, Si: 0.6 to 0.8%, Mn: 0.7 to 0.9%, S: 0.01 to 0.05%, Mo: 0.3 to 0.5%, B: 0.0005 to 0.005%, Al: 0.002 to 0.05%, and Ti: 0.02 to 0.09%, restricting N to 0.007% or less, Cr to 0.15% or less, and P to 0.02% or less, having a structural percentage of bainite + martensite of 40% or more, and having a hardness of 250 to 340HV and a high strength constant velocity joint intermediate shaft made of that steel material, having a spline-vanishing part with a surface hardness of 610 to 750HV and a ratio t/r of an effective hardened layer depth t and radius r of 0.35 to 0.55, having a flat part with a surface hardness of 630 to 770HV and a ratio t/r of an effective hardened layer depth t and radius r of 0.55 to 1.0, and having a core hardness of 250 to 340HV.

    摘要翻译: C:0.46〜0.52%,Si:0.6〜0.8%,Mn:0.7〜0.9%,S:0.01〜0.05%,Mo:0.3〜0.5%的高强等速万向节中间轴用钢材,B: 0.0005〜0.005%,Al:0.002〜0.05%,Ti:0.02〜0.09%,N:0.007%以下,Cr:0.15%以下,P:0.02%以下,贝氏体+ 40%以上的马氏体,硬度为250〜340HV,由该钢材制成的高强度等速万向节中间轴,具有表面硬度为610〜750HV的花键消失部,比率t / r 的有效硬化层d