Process for preparation of aluminum borate whisker
    1.
    发明公开
    Process for preparation of aluminum borate whisker 失效
    制备硼酸铝清洗剂的方法

    公开(公告)号:EP0375325A3

    公开(公告)日:1990-11-14

    申请号:EP89313210.0

    申请日:1989-12-18

    IPC分类号: C30B1/10 C30B29/10 C30B29/62

    CPC分类号: C30B1/10 C30B29/10 C30B29/62

    摘要: A mixture comprising (i) an oxide, hydroxide or oxyhydroxide of aluminum, (ii) an aluminum-containing sulfate, (iii) an oxide or oxyacid of boron or an alkali metal salt thereof and (iv) an alkali metal sulfate is heated at a temperature of 900 to 1200° C to grow an aluminum borate whisker. In this process, the reaction is advanced apparently in the solid phase, and this process is advantageous over the conventional processes in that the yield is high and the isolation and purification of the reaction product is facilitated.

    摘要翻译: 一种混合物,其包含(i)铝的氧化物,氢氧化物或羟基氧化铝,(ii)含铝硫酸盐,(iii)硼的氧化物或含氧酸或其碱金属盐和(iv)碱金属硫酸盐的混合物在 在900〜1200℃的温度下生长硼酸铝晶须。 在该方法中,反应显然在固相中进行,并且该方法优于常规方法,因为产率高,反应产物的分离和纯化变得容易。

    Process for preparation of aluminium borate whisker
    2.
    发明公开
    Process for preparation of aluminium borate whisker 失效
    硼酸铝晶须的制备方法

    公开(公告)号:EP0375354A2

    公开(公告)日:1990-06-27

    申请号:EP89313270.4

    申请日:1989-12-19

    IPC分类号: C30B1/10 C30B29/10 C30B29/62

    CPC分类号: C30B1/10 C30B29/10 C30B29/62

    摘要: An aluminum borate whisker is prepared by heating and reacting aluminum sulfate and an oxide of boron, an oxyacid of boron or an alkali metal salt thereof in the presence of an alkali metal sulfate and an alkali metal carbonate. In this process, the reaction is advanced apparently in the solid phase, and this process is advantageous over the conventional processes in that the yield is high and the withdrawal of the reaction product is facilitated.

    摘要翻译: 通过在碱金属硫酸盐和碱金属碳酸盐的存在下加热硫酸铝和硼的氧化物,硼的含氧酸或其碱金属盐并使其反应来制备硼酸铝晶须。 在该过程中,反应显着地在固相中进行,并且与常规方法相比,该方法的优点在于收率高并且促进了反应产物的取出。

    Process for preparation of aluminum borate whisker
    3.
    发明公开
    Process for preparation of aluminum borate whisker 失效
    Verfahren zur Herstellung von铝 - Borat-Whiskern。

    公开(公告)号:EP0375325A2

    公开(公告)日:1990-06-27

    申请号:EP89313210.0

    申请日:1989-12-18

    IPC分类号: C30B1/10 C30B29/10 C30B29/62

    CPC分类号: C30B1/10 C30B29/10 C30B29/62

    摘要: A mixture comprising (i) an oxide, hydroxide or oxyhydroxide of aluminum, (ii) an aluminum-containing sulfate, (iii) an oxide or oxyacid of boron or an alkali metal salt thereof and (iv) an alkali metal sulfate is heated at a temperature of 900 to 1200° C to grow an aluminum borate whisker. In this process, the reaction is advanced apparently in the solid phase, and this process is advantageous over the conventional processes in that the yield is high and the isolation and purification of the reaction product is facilitated.

    摘要翻译: 一种混合物,其包含(i)铝的氧化物,氢氧化物或羟基氧化铝,(ii)含铝硫酸盐,(iii)硼的氧化物或含氧酸或其碱金属盐和(iv)碱金属硫酸盐的混合物在 在900〜1200℃的温度下生长硼酸铝晶须。 在该方法中,反应显然在固相中进行,并且该方法优于常规方法,因为产率高,反应产物的分离和纯化变得容易。

    Process for preparation of aluminium borate whisker
    4.
    发明公开
    Process for preparation of aluminium borate whisker 失效
    制备硼酸铝清洗剂的方法

    公开(公告)号:EP0375354A3

    公开(公告)日:1990-11-22

    申请号:EP89313270.4

    申请日:1989-12-19

    IPC分类号: C30B1/10 C30B29/10 C30B29/62

    CPC分类号: C30B1/10 C30B29/10 C30B29/62

    摘要: An aluminum borate whisker is prepared by heating and reacting aluminum sulfate and an oxide of boron, an oxyacid of boron or an alkali metal salt thereof in the presence of an alkali metal sulfate and an alkali metal carbonate. In this process, the reaction is advanced apparently in the solid phase, and this process is advantageous over the conventional processes in that the yield is high and the withdrawal of the reaction product is facilitated.

    摘要翻译: 通过在碱金属硫酸盐和碱金属碳酸盐的存在下,使硫酸铝和硼的氧化物,硼的含氧酸或其碱金属盐加热和反应来制备硼酸铝晶须。 在该方法中,反应明显地在固相中进行,并且该方法相对于常规方法是有利的,因为产率高并且促进反应产物的排出。